Environmentally friendly putty
A technology of atomic ash and environmental protection, which is applied in the direction of filling slurry, etc., can solve the problems of insufficient performance and requirements, and achieve the effects of good environmental protection performance, good construction and use performance, and good matching performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] An environment-friendly putty, the putty is composed of two components: main body and curing agent, when used, the weight ratio is main body: curing agent = 100: 2, just mix evenly; the main body is composed of the following parts by weight: The composition of the ingredients: 56 parts of air-drying water-based unsaturated polyester resin, 5 parts of styrene, 0.5 parts of triethylenetetramine, 1.2 parts of dimethylaniline, 1.2 parts of polymethyl methacrylate, 1.6 parts of BYK-980, 0.01 part of dimethylglyoxime, 0.025 part of polyamide wax, 0.2 part of methyl paraben, 8 parts of hollow glass microspheres, 1 part of bentonite, 7 parts of calcium carbonate, 10 parts of titanium dioxide, 2 parts of glass fiber, 3 parts of barium sulfate The curing agent consists of the following components by weight ratio: 64 parts of benzoyl peroxide, 20 parts of dibutyl phthalate, and 8 parts of silicon dioxide.
Embodiment 2
[0019] An environment-friendly putty, the putty is composed of two components: main body and curing agent, when used, the weight ratio is main body: curing agent = 100: 2, just mix evenly; the main body is composed of the following parts by weight: The composition of the above ingredients: 60 parts of air-drying water-based unsaturated polyester resin, 2 parts of styrene, 0.8 parts of triethylenetetramine, 0.8 parts of dimethylaniline, 1.5 parts of polymethyl methacrylate, 1.2 parts of BYK-980, 0.02 parts of dimethylglyoxime, 0.015 parts of polyamide wax, 0.3 parts of methyl paraben, 4 parts of hollow glass microspheres, 3 parts of bentonite, 5 parts of calcium carbonate, 15 parts of titanium dioxide, 1 part of glass fiber, 5 parts of barium sulfate The curing agent consists of the following components by weight: 60 parts of benzoyl peroxide, 24 parts of dibutyl phthalate, and 4 parts of silicon dioxide.
Embodiment 3
[0021] An environment-friendly putty, the putty is composed of two components: main body and curing agent, when used, the weight ratio is main body: curing agent = 100: 2, just mix evenly; the main body is composed of the following parts by weight: The composition of the above ingredients: 57 parts of air-drying water-based unsaturated polyester resin, 4 parts of styrene, 0.6 parts of triethylenetetramine, 1.1 parts of dimethylaniline, 1.3 parts of polymethyl methacrylate, 1.5 parts of BYK-980, 0.014 parts of dimethylglyoxime, 0.022 parts of polyamide wax, 0.22 parts of methyl paraben, 7 parts of hollow glass microspheres, 1.5 parts of bentonite, 6.5 parts of calcium carbonate, 12 parts of titanium dioxide, 1.6 parts of glass fiber, 3.5 parts of barium sulfate The curing agent consists of the following components by weight: 63 parts of benzoyl peroxide, 21 parts of dibutyl phthalate, and 7 parts of silicon dioxide.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com