[0017] The present invention can be realized by the following steps in implementation:
[0018] 1, preparation treatment liquid: described treatment liquid comprises zinc dipping liquid, pre-copper plating liquid, copper plating liquid, and zinc dipping liquid is made of zinc oxide 100g, sodium hydroxide 500g, iron trichloride 3g, potassium sodium tartrate 10g, Water, wherein, first dissolve sodium hydroxide in 500ml water, stir continuously until fully dissolved, then add zinc oxide, heat until fully dissolved to form solution A, dissolve ferric chloride and potassium sodium tartrate in a small amount of water, To form solution B, mix solution A and solution B, add water to 1000ml and mix well;
[0019] The pre-copper plating solution is made of 35g of cuprous cyanide, 7g of sodium cyanide, and water. Dissolve sodium cyanide in a small amount of water, then add cuprous cyanide to dissolve it, add water to 1000ml and mix well;
[0020] The copper plating solution is made of p...
Embodiment 2
[0026] The present invention can be realized by the following steps:
[0027] 1, preparation treatment liquid: described treatment liquid comprises zinc dipping liquid, pre-copper plating liquid, copper plating liquid, and zinc dipping liquid is made of zinc oxide 100g, sodium hydroxide 500g, iron trichloride 3g, potassium sodium tartrate 10g, Water, wherein, first dissolve sodium hydroxide in 500ml water, stir continuously until fully dissolved, then add zinc oxide, heat until fully dissolved to form solution A, dissolve ferric chloride and potassium sodium tartrate in a small amount of water, To form solution B, mix solution A and solution B, add water to 1000ml and mix well;
[0028] The pre-plating copper solution is made of 38g of cuprous cyanide, 7.5g of sodium cyanide, and water. Dissolve sodium cyanide in a small amount of water, then add cuprous cyanide to dissolve it, add water to 1000ml and mix well;
[0029] The copper plating solution is made of potassium pyropho...
Embodiment 3
[0035] The present invention can also be realized by the following steps:
[0036] 1, preparation treatment liquid: described treatment liquid comprises zinc dipping liquid, pre-copper plating liquid, copper plating liquid, and zinc dipping liquid is made of zinc oxide 100g, sodium hydroxide 500g, iron trichloride 3g, potassium sodium tartrate 10g, Water, wherein, first dissolve sodium hydroxide in 500ml water, stir continuously until fully dissolved, then add zinc oxide, heat until fully dissolved to form solution A, dissolve ferric chloride and potassium sodium tartrate in a small amount of water, To form solution B, mix solution A and solution B, add water to 1000ml and mix well;
[0037] The pre-copper plating solution is made of 40g of cuprous cyanide, 8g of sodium cyanide, and water. Dissolve sodium cyanide in a small amount of water, then add cuprous cyanide to dissolve it, add water to 1000ml and mix well;
[0038] The copper plating solution is made of potassium pyro...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com