Aqueous fire retardation antirust coating material

A kind of anti-rust coating, water-based technology, applied in the field of coatings, can solve problems such as the decline of bearing capacity and balance stability, endanger the health of users, damage the ecological environment, etc., achieve strong adhesion, wide application range, and overcome pollution effects

Inactive Publication Date: 2013-11-27
WUJIANG JUNDA ELEVATOR PARTS
View PDF6 Cites 11 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, at present, most of the paints are solvent-based paints, which contain about 50% organic solvents. These paints will release a large amount of VOC gas after spraying, which not only seriously endangers the health of users, but also pollutes the atmosphere. , damage the ecological environment
[0004] Although metal is a non-combustible material, its mechanical index will change greatly with the change of temperature, and its bearing capacity and balance stability will drop significantly with the increase of temperature.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Aqueous fire retardation antirust coating material

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0014] A water-based flame-retardant anti-rust coating, characterized in that it comprises the following raw materials in parts by weight: 100 parts of styrene-acrylic emulsion, 8 parts of epoxy resin, 15 parts of glass flakes, 0.1 part of zinc phosphate, dimethyl phosphonate 4 parts of ester, 2 parts of aluminum tripolyphosphate, 0.5 part of sorbitan monooleate, 0.2 part of nonylphenol polyoxyethylene ether, 0.1 part of triethylamine, 0.1 part of sodium hexametaphosphate, polyether modified Silicone oil 0.1 part, deionized water 10 parts.

[0015] The production method of the water-based flame-retardant and anti-rust coating of the present embodiment is obtained by mixing, stirring and removing impurities from the above-mentioned raw materials by physical methods.

Embodiment 2

[0017] A water-based flame-retardant anti-rust paint, characterized in that it includes the following raw materials in parts by weight: 120 parts of styrene-acrylic emulsion, 10 parts of epoxy resin, 25 parts of glass flakes, 0.3 parts of zinc phosphate, dimethyl phosphonate 10 parts of ester, 4 parts of aluminum tripolyphosphate, 2 parts of sorbitan monooleate, 0.3 part of nonylphenol polyoxyethylene ether, 0.2 part of triethylamine, 1 part of sodium hexametaphosphate, polyether modified 0.5 parts of silicone oil, 20 parts of deionized water.

[0018] The production method of the water-based flame-retardant and anti-rust coating of the present embodiment is obtained by mixing, stirring and removing impurities from the above-mentioned raw materials by physical methods.

[0019]

Embodiment 3

[0021] A water-based flame-retardant and anti-rust coating is characterized in that it includes the following raw materials in parts by weight: 110 parts of styrene-acrylic emulsion, 9 parts of epoxy resin, 20 parts of glass flakes, 0.2 part of zinc phosphate, dimethyl phosphonate 8 parts of ester, 3 parts of aluminum tripolyphosphate, 1.2 parts of sorbitan monooleate, 0.25 parts of nonylphenol polyoxyethylene ether, 0.14 parts of triethylamine, 0.7 parts of sodium hexametaphosphate, polyether modified 0.3 parts of silicone oil, 15 parts of deionized water.

[0022] The production method of the water-based flame-retardant and anti-rust coating of the present embodiment is obtained by mixing, stirring and removing impurities from the above-mentioned raw materials by physical methods.

[0023]

[0024] Product performance of the present invention is tested according to national standards, and its test results are as shown in Table 1.

[0025]

[0026] Table 1 Product performa...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The present invention relates to an aqueous fire retardation antirust coating material, which is characterized by comprising the following raw materials, by weight: 100-120 parts of a styrene-acrylate emulsion, 8-10 parts of an epoxy resin, 15-25 parts of glass flakes, 0.1-0.3 part of zinc phosphate, 4-10 parts of dimethyl methylphosphonate, 2-4 parts of aluminum tripolyphosphate, 0.5-2 parts of sorbitan monooleate, 0.2-0.3 part of polyoxy ethylene nonyl phenyl ether, 0.1-0.2 part of triethylamine, 0.1-1 part of a dispersing agent, 0.1-0.5 part of an antifoaming agent, and 10-20 parts of deionized water. The product has characteristics of good corrosion resistance, strong adhesion to the substrate, substrate protection, rust resistance and good fire retardation, adopts water as a solvent so as to overcome pollution of the solvent type coating material on the environment, and is a green environmental protection coating material.

Description

technical field [0001] The invention belongs to the technical field of coatings, and in particular relates to a water-based flame-retardant anti-rust coating. Background technique [0002] The problem of metal corrosion pervades all walks of life in the national economy. It will cause great damage to the performance and commercial value of metal products, and even cause major failures and make equipment scrapped. Therefore, the problem of metal rust prevention has increasingly attracted people. s concern. [0003] Applying anti-corrosion coatings is the most economical and effective anti-corrosion method. However, at present, most of the paints are solvent-based paints, which contain about 50% organic solvents. These paints will release a large amount of VOC gas after spraying, which not only seriously endangers the health of users, but also pollutes the atmosphere. , damaging the ecological environment. [0004] Although metal is a non-combustible material, its mechanica...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D125/14C09D163/00C09D5/08C09D5/18
Inventor 平利中
Owner WUJIANG JUNDA ELEVATOR PARTS
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products