Medical stone water-soluble mineral silicon fertilizer
A technology of medical stone water and medical stone silicate, which is applied in the direction of fertilization equipment, fertilizer mixture, application, etc., can solve the problems of inability to be absorbed by crops, low activity and water solubility, and poor water solubility, so as to achieve good absorption and increase Thickness, the effect of reducing the dosage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] 1: The number of medical stone mineral powder is 600-800 mesh, the medical stone mineral powder accounts for 65-70% of the total weight of the two, and the input ratio is 30-35% potassium hydroxide. Calcined at a high temperature of 1200-2000 for 1 hour while hot, quenched in water, settled, and concentrated to obtain silicate crystals containing various minerals. The silicate crystals were determined to contain silicon dioxide 60 %, and contains boron, selenium, and rare earth elements such as lanthanum, cerium, and more than 50 kinds of trace elements needed by plants.
[0030] 2. Take 600 kg of medical stone silicic acid crystals and put them into the reaction kettle, add 400 kg of water for more than 3 pressures (MP) 80-120°C to completely melt, filter to remove insoluble matter, and cool the liquid at room temperature for use.
Embodiment 2
[0044] Step 1: The medical stone mineral powder has a mesh number of 600 mesh, the medical stone mineral powder accounts for 65%, and the input accounts for 32% of potassium hydride dissolved water. Calcined at 1400°C for 1 hour while hot, quenched in water, settled, and concentrated to obtain silicate crystals containing various minerals. The silicate crystals contain 60% silicon dioxide as determined by microspectroscopy and X-ray diffractometer More than 50 kinds of trace elements required by plants such as boron, selenium, and rare earth elements lanthanum, cerium, etc.
[0045] Step 2: Take 600 kg of medical stone silicic acid crystals and put them into the reaction kettle, add 400 kg of water and over 3 pressures (MP) at 100°C to completely melt, filter to remove insoluble matter, and cool the liquid at room temperature for use.
[0046] Step 3: Two-way chelation: Take 15 kg of zinc oxide, 5 kg of manganese nitrate, and 3 kg of ammonium molybdate, dissolve them in 300°C ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com