Fibrous gypsum imitation antifreeze really stone paint and using method
A technology of real stone paint and imitation marble, applied in the field of coatings, can solve problems such as erosion of stone itself, geological structure, waste of geological resources, hidden dangers of construction safety, etc., to save the use of non-renewable resources, reduce nighttime construction behavior, and improve construction. The effect of efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] The purpose of this embodiment is to provide a kind of imitation stone antifreeze real stone paint and its application method.
[0049]This embodiment specifically provides a kind of imitation stone antifreeze real stone paint, in addition to colored sand and pH adjuster, the colloid is also composed of the following components in mass fraction: water 20~70%, antifreeze material 10~50%, emulsion 10.5~12.0%, cellulose 0.05~0.25%, film-forming aid 0.05~0.20%, ethylene glycol 0.45~0.70%, defoamer 0.05~0.20%, fungicide 0.05~0.20%; the quality of colloid and colored sand The ratio is 1:3 to 1:4;
[0050] The method for preparing imitation marble antifreeze real stone paint:
[0051] a. Mix water and cellulose with a mass ratio of 30% and stir for 30 to 50 minutes, and the stirring speed is 800 to 1500 revolutions per minute;
[0052] b. Add the remaining water, film-forming aids, ethylene glycol, defoamer, and methanol in sequence, and stir at a constant speed at a speed o...
Embodiment 2
[0090] A kind of imitation marble antifreeze real stone paint of the present embodiment, is made up of colloid by the component of following mass fraction:
[0091] Water 43.15%, methanol 45%, KT01 emulsion 11.0%, hydroxypropyl methylcellulose 0.15%, alcohol ester twelve film-forming aids 0.05%, ethylene glycol 0.55%, defoamer 0.05%, bactericide 0.05% ; The mass mixing ratio of colloid and colored sand is 1:3; the pH regulator is phosphoric acid and sodium dihydrogen phosphate. The colored sand is 20 mesh black and white sand. The colored sand in this embodiment is colored sand produced by crushing waste marble.
[0092] The method for preparing imitation marble antifreeze real stone paint:
[0093] Mix water and cellulose with a mass ratio of 30% and stir for 40 minutes, and the stirring speed is 1200 rpm; after the remaining water, film-forming aids, ethylene glycol, defoamer, and methanol are sequentially mixed, the stirring speed is 1200 rpm. Stir at a constant speed of...
Embodiment 3
[0097] A kind of imitation marble antifreeze real stone paint of the present embodiment, is made up of colloid by the component of following mass fraction:
[0098]Water 57.4%, methanol 30%, KT01 emulsion 11.5%, hydroxypropyl methylcellulose 0.20%, alcohol ester twelve film-forming aids 0.10%, ethylene glycol 0.60%, defoamer 0.1%, bactericide 0.1% ; The mass mixing ratio of colloid and colored sand is 1:4; the pH regulator is hydrochloric acid and potassium hydroxide. The colored sand is 30 mesh black sand and pink sand. The colored sand in this embodiment is marble powder produced during the marble processing.
[0099] The method for preparing imitation marble antifreeze real stone paint:
[0100] Take 40% water and cellulose by mass and mix and stir for 30 minutes at a stirring speed of 1000 revolutions per minute; after the remaining water, film-forming aids, ethylene glycol, defoamer and methanol are sequentially mixed, the stirring speed is 1000 revolutions per minute. ...