A processing technology and technology of dough skin, applied in the direction of leather surface treatment, leather surface mechanical treatment, small raw hide/large raw hide/leather/fur treatment, etc., can solve the problem of poor wear resistance and scratch resistance, waste of resources and property , reduce the leather usage rate and other issues, to achieve the effect of maintaining the overall effect, prolonging the service life, and simple and easy operation steps
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A kind of color fast waterproof nubuck leather surface processing technology, specifically comprises the following steps:
[0022] (1) Cleaning For lightly soiled nubuck leather garments, use sandpaper to polish the blackened and bright parts, and smooth the fleece to make it fluff up, and then spray the color restoration agent; for heavily soiled nubuck leather, use Use hot water at 70-80°C to emulsify the special cleaning agent. Use a medium-soft brush to dip the emulsified special cleaning agent to scrub the surface and inner skirt. After rinsing and drying, gently stretch the upper leather to avoid Wrinkled;
[0023] (2) Nubuck: The surface of the cleaned upper leather is buffed, and the buffing equipment adopts a tension buffing machine, a gap buffing machine or a continuous buffing machine, and the coating is ground by 0.05~0.15mm;
[0024] (3) Spray filler Adjust the amount of filler sprayed according to the position difference of the upper leather to reduce the...
Embodiment 2
[0033] The difference in Example 1 is that the specific components of the filler in the step (3) include 10 parts of capric triglyceride, 2 parts of ethylene glycol, 6 parts of silicone additives, 4 parts of metal aluminum powder, silicone 15 parts of modified polyurethane resin, 5 parts of defoaming and smoothing agent SAF, 6 parts of silane coupling agent, 3 parts of Span, 6 parts of glycerin, 3 parts of chain extender, and 38 parts of solvent. The solvent includes 3 parts of butyl acetate, 6 parts of cyclohexanone, and 2 parts of ethylene glycol butyl ether.
Embodiment 3
[0035] The difference from Example 1 is that the specific ingredients of the filler in the step (3) include 12 parts of capric triglyceride, 2 parts of ethylene glycol, 7 parts of silicone additives, 5 parts of metal aluminum powder, organic 18 parts of silicon-modified polyurethane resin, 5 parts of defoaming smoothing agent SAF, 7 parts of silane coupling agent, 4 parts of Span, 12 parts of glycerin, 5 parts of chain extender, and 45 parts of solvent. The solvent includes 5 parts of butyl acetate, 8 parts of cyclohexanone, and 3 parts of ethylene glycol butyl ether.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com