A technology of electroplating wastewater and flocculant, which is applied in metallurgical wastewater treatment, chemical instruments and methods, flocculation/sedimentation water/sewage treatment, etc., can solve the problems of high investment cost, long treatment process and complicated treatment process, and meet the requirements of Water intake requirements, fast sedimentation speed, and good treatment effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The compound flocculant is compounded by hydrogen peroxide, polyaluminum chloride, aluminum sulfate and cerium sulfate in a molar ratio of 1:5:2:1, and water is added to make a solution with a mass fraction of 5%.
[0024] Add the compounded flocculant to the electroplating phosphorus-containing fluorine-containing wastewater, where the total phosphorus content is 2.5mg / L, the fluorine content is 15.2mg / L, the amount of flocculant added is 50mg / L, and the speed is 160rpm. After stirring for 1 minute, use 50rpm slow stirring for 20 minutes. After standing for 30 minutes, the concentration of phosphorus and fluorine in the supernatant was measured. The results showed that the total phosphorus concentration in the wastewater treated with the compound flocculant was 0.19mg / L, and the fluoride concentration It is 1.8mg / L, which meets the requirements of reverse osmosis membrane.
Embodiment 2
[0026] The compound flocculant is compounded by hydrogen peroxide, polyaluminum chloride, aluminum nitrate and cerium nitrate in a molar ratio of 1:10:5:2, and water is added to make a solution with a mass fraction of 20%.
[0027] Add the compounded flocculant to the electroplating phosphorous-containing fluorine-containing wastewater. The total phosphorus content is 5.0mg / L, the fluorine content is 18.9mg / L, and the amount of flocculant added is 150mg / L. After stirring and precipitation , The concentration of phosphorus and fluorine in the supernatant was measured, and the results showed that the total phosphorus concentration in the wastewater after treatment with the compound flocculant was 0.15mg / L, and the fluoride concentration was 1.6mg / L, which met the requirements for the reverse osmosis membrane.
Embodiment 3
[0029] The compound flocculant is compounded by hydrogen peroxide, polyaluminum chloride, aluminum chloride and cerium chloride in a molar ratio of 1:8:4:1, and water is added to make a solution with a mass fraction of 16%.
[0030] Add the compounded flocculant to the electroplating wastewater containing phosphorous and fluorine. The total phosphorus content is 4.2mg / L, the fluorine content is 20.0mg / L, and the amount of flocculant added is 300mg / L. After stirring and precipitation , The concentration of phosphorus and fluorine in the supernatant was measured, and the results showed that the total phosphorus concentration in the wastewater treated with the compound flocculant was 0.30mg / L and the fluoride concentration was 1.2mg / L, which met the requirements for the reverse osmosis membrane.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com