Examples
Embodiment 1
[0017] Environmentally friendly paint for the surface of kitchen furniture, prepared from the following raw materials in parts by weight: 20 parts of alkyd resin, 14 parts of polyamide resin, 6 parts of butyl acetate, 30 parts of acrylic emulsion, 80 parts of weakly acidic water, ethylene glycol 12 parts of alcohol, 4 parts of castor oil, 1.2 parts of glass powder, 0.6 parts of titanium dioxide, 0.3 parts of nano silver oxide, 0.8 parts of carboxymethyl cellulose, 6 parts of dispersant, 6 parts of pentaerythritol, 4 parts of limonene, zinc epoxy acid 1 serving.
[0018] The preparation steps of above-mentioned environmental protection paint are as follows:
[0019] (1) Add weakly acidic water into the mixer at a speed of 400 rpm, then add alkyd resin, polyamide resin, and butyl acetate sequentially every 20 minutes, and stir for 40 minutes after adding to fully react;
[0020] (2) Add acrylic acid emulsion, ethylene glycol, and castor oil sequentially every 10 minutes, and st...
Embodiment 2
[0025] Environmentally friendly paint for the surface of kitchen furniture, prepared from the following raw materials in parts by weight: 25 parts of alkyd resin, 12 parts of polyamide resin, 8 parts of butyl acetate, 25 parts of acrylic emulsion, 90 parts of weakly acidic water, ethylene glycol 10 parts of alcohol, 5 parts of castor oil, 1 part of glass powder, 0.7 parts of titanium dioxide, 0.25 parts of nano silver oxide, 1 part of carboxymethyl cellulose, 5 parts of dispersant, 7 parts of pentaerythritol, 3.5 parts of limonene, zinc epoxy acid 1.5 servings.
[0026] The preparation steps of above-mentioned environmental protection paint are as follows:
[0027] (1) Add weakly acidic water into the agitator at a speed of 450 rpm, then add alkyd resin, polyamide resin, and butyl acetate sequentially every 22 minutes, and stir for 50 minutes after adding to fully react;
[0028] (2) Add acrylic acid emulsion, ethylene glycol, and castor oil sequentially every 11 minutes, and...
Embodiment 3
[0033] Environmentally friendly paint for the surface of kitchen furniture, prepared from the following raw materials in parts by weight: 30 parts of alkyd resin, 10 parts of polyamide resin, 10 parts of butyl acetate, 20 parts of acrylic emulsion, 100 parts of weakly acidic water, ethylene glycol 8 parts of alcohol, 6 parts of castor oil, 0.8 parts of glass powder, 0.8 parts of titanium dioxide, 0.2 parts of nano silver oxide, 1.2 parts of carboxymethyl cellulose, 4 parts of dispersant, 8 parts of pentaerythritol, 3 parts of limonene, zinc epoxy acid 2 servings.
[0034] The preparation steps of above-mentioned environmental protection paint are as follows:
[0035] (1) Add weakly acidic water into the mixer at a speed of 500 rpm, then add alkyd resin, polyamide resin, and butyl acetate sequentially every 24 minutes, and stir for 60 minutes after adding to fully react;
[0036] (2) Add acrylic acid emulsion, ethylene glycol, and castor oil sequentially every 12 minutes, and ...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com