A scale inhibitor and slow-release technology, applied in the field of strip-shaped slow-release scale inhibitor and its preparation, can solve the problems of unstable scale inhibition performance, complicated regeneration operation, low water utilization rate, etc. Mechanical strength, effect of zero-emission maintenance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A bar-shaped slow-release antiscaling agent is made of the following components in terms of weight percentage: polyaspartic acid: 45%, sodium carboxymethylcellulose: 20% and water: 35%. The preparation steps of the slow-release scale inhibitor include:
[0023] 1) polyaspartic acid, sodium carboxymethylcellulose and water of the above weight are fully stirred and mixed in a mixer to form a uniform plastic body;
[0024] 2) Extrude the plastomer in step 1) in an extruder to obtain a solid cylindrical slow-release scale inhibitor wet material with a length of 10mm and a diameter of 1.5mm, and place the wet material in an oven at 80°C Dry for 10 hours to obtain the strip-shaped slow-release scale inhibitor.
Embodiment 2
[0026] A bar-shaped slow-release antiscalant is made of the following components in terms of weight percentage: polyepoxysuccinic acid: 20%, tannin: 30%, cyclodextrin: 15% and water: 35%. The preparation steps of the slow-release scale inhibitor include:
[0027] 1) The polyepoxysuccinic acid, tannin, cyclodextrin and water of the above weight are fully stirred and mixed in a mixer to form a uniform plastic body;
[0028] 2) Extrude the plastomer in step 1) in an extruder to obtain a solid cylindrical slow-release scale inhibitor wet material with a length of 15mm and a diameter of 2.5mm, and place the wet material in an oven at 100°C Dry for 8 hours to obtain the strip-shaped slow-release scale inhibitor.
Embodiment 3
[0030] A strip-shaped slow-release antiscalant, which is made of the following components by weight percentage: starch: 20%, lignin: 20%, chitosan: 15%, scallion powder: 15% and water: 30%. The preparation steps of the slow-release scale inhibitor include:
[0031] 1) fully stir and mix the starch, lignin, chitosan, safflower powder and water of the above-mentioned weight in a mixer to form a uniform plastic body;
[0032] 2) Extrude the plastomer in step 1) in an extruder to obtain a solid cylindrical slow-release scale inhibitor wet material with a length of 20mm and a diameter of 2.0mm, and place the wet material in an oven at 120°C Dry for 4 hours to obtain the strip-shaped slow-release scale inhibitor.
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com