Antibacterial plastic for automobile interior parts, and preparation method thereof
A technology for automotive interior parts and antibacterial plastics, applied in the field of antibacterial plastics for automotive interior parts and its preparation, can solve problems such as air pollution, achieve fast performance, and solve the effect of slow sterilization speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] This antibacterial plastic for automotive interior parts includes the following raw materials: 40 kg of polycarbonate, 40 kg of polyamide, 2 kg of nano-zinc oxide, 2 kg of anatase titanium dioxide, 1 kg of zinc stearate, 1 kg of barium laurate, carbon Black 1kg, titanium dioxide 2kg, dioctyl phthalate 0.5 kg, didodecyl thiodipropionate 0.5 kg, hindered phenol phosphate 0.3 kg, calcium carbonate 5 kg, calcium silicate 5 kg.
[0017] The preparation method is to weigh each component according to the proportion, mix uniformly, melt and knead, extrude and granulate.
[0018] The antibacterial rate of the antibacterial plastic prepared in this embodiment is 99.11.
Embodiment 2
[0020] This kind of antibacterial plastic for automotive interior parts includes the following raw materials: 40 kg of polyethylene, 40 kg of polyamide, 20 kg of polyphenylene ether, 4 kg of nano-zinc oxide, 4 kg of anatase titanium dioxide, 1 kg of barium stearate, hard Zinc fatty acid 1 kg, zinc oxide 1 kg, plasticizer hindered phenol phosphate salt 0.5 kg, phosphite antioxidant 0.3 kg, tris(2,4-di-tert-butylphenyl) phosphite 0.5 kg, ortho 0.3 kg of diisobutyl phthalate, 5 kg of glass fiber with a length of 12-25 mm, 5 kg of calcium carbonate, and 5 kg of mica.
[0021] The preparation method is the same as in Example 1.
[0022] The antibacterial rate of the antibacterial plastic prepared in this embodiment is 99.24.
Embodiment 3
[0024] This kind of antibacterial plastic for automotive interior parts includes the following raw materials: polyimide 20 kg, polyphenylene sulfide 40 kg, polybenzimidazole 40 kg, nano-zinc oxide 2 kg, anatase titanium dioxide 4 kg, castor oil Barium acid 1 kg, zinc stearate 1 kg, nickel complex compound 2002 0.2 kg, butyl benzyl phthalate 0.5 kg, dioctyl phthalate 0.5 kg, dibutyl hydroxytoluene 0.5 kg, 0.3 kg of phenolic phosphate ester salt, 0.3 kg of didodecyl thiodipropionate; 5 kg of glass fiber with a length of 12-25 mm, and 10 kg of calcium carbonate.
[0025] The preparation method is the same as in Example 1.
[0026] The antibacterial rate of the antibacterial plastic prepared in this embodiment is 99.13.
PUM
| Property | Measurement | Unit |
|---|---|---|
| antibacterial rate | aaaaa | aaaaa |
| antibacterial rate | aaaaa | aaaaa |
| antibacterial rate | aaaaa | aaaaa |