Desizing treatment method for cotton-polyester blended fabric

A technology of cotton-polyester blending and processing methods, which is applied in the direction of textiles, papermaking, and dry-cleaning fiber products. It can solve problems such as hindering the contact between dyeing materials and fibers, affecting the quality of printing and dyeing products, and unfavorable printing and dyeing processing, so as to ensure the quality of subsequent printing and dyeing. Improves the effect of hand feel, high hair effect and mechanical properties

Inactive Publication Date: 2018-03-23
SHANGHAI WOO BRAND MANAGEMENT CO LTD
View PDF0 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Sizing on gray cloth is unfavorable to printing and dyeing processing, because the existence of sizing will contaminate the finishing fluid, consume dyeing materials, and even hinder the contact between dyeing materials and fibers, affecting the quality of printing and dyeing products

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0023] 1) Preparation of desizing solution: 2 parts by weight of sodium citrate, 0.85 parts by weight of hydrogen peroxide, 0.85 parts by weight of N-methylpyrrolidone, 1 part by weight of isomeric fatty alcohol polyoxyethylene ether phosphate, 1.3 parts by weight of barium petroleum sulfonate , 2 parts by weight of sodium hydroxide, and 21 parts by weight of amylase are dropped into 50 parts by weight of deionized water successively, and stirred evenly; Oxyethylene ether, 0.65 parts by weight of octadecyl dimethyl ammonium chloride, continue to stir until fully mixed, and obtain a desizing solution;

[0024] 2) Fabric pretreatment: Soak the fabric in warm water at 45°C. When soaking, the warm water needs to cover the fabric. Add acetic acid during the soaking process to adjust the pH value of the warm water to 5.5. After the adjustment is completed, stir the fabric for 10 minutes. Take it out after completion;

[0025] 3) Dehydration of the fabric, the fabric fished out in s...

Embodiment 2

[0032] 1) Preparation of desizing solution: 2 parts by weight of sodium citrate, 0.85 parts by weight of hydrogen peroxide, 1.2 parts by weight of N-methylpyrrolidone, 1.6 parts by weight of isomeric fatty alcohol polyoxyethylene ether phosphate, 1.3 parts by weight of barium petroleum sulfonate , 2.32 parts by weight of sodium hydroxide, and 21 parts by weight of amylase are dropped into 55 parts by weight of deionized water successively, and stirred evenly; Oxyethylene ether, 0.65 parts by weight of octadecyl dimethyl ammonium chloride, continue to stir until fully mixed, and obtain a desizing solution;

[0033] 2) Fabric pretreatment: Soak the fabric in warm water at 30°C. When soaking, the warm water needs to cover the fabric. Add acetic acid during the soaking process to adjust the pH value of the warm water to 5. After the adjustment is completed, stir the fabric for 15 minutes. Take it out after completion;

[0034] 3) Dehydration of the fabric, the fabric fished out i...

Embodiment 3

[0041]1) Preparation of desizing solution: 1.6 parts by weight of sodium citrate, 0.8 parts by weight of hydrogen peroxide, 1 part by weight of N-methylpyrrolidone, 1.3 parts by weight of isomeric fatty alcohol polyoxyethylene ether phosphate, 1.23 parts by weight of barium petroleum sulfonate , 2.1 parts by weight of sodium hydroxide, and 20 parts by weight of amylase are dropped into 53 parts by weight of deionized water successively, and stirred evenly; Oxyethylene ether, 0.65 parts by weight of octadecyl dimethyl ammonium chloride, continue to stir until fully mixed, and obtain a desizing solution;

[0042] 2) Fabric pretreatment: Soak the fabric in warm water at 45°C. When soaking, the warm water needs to cover the fabric. Add acetic acid during the soaking process to adjust the pH value of the warm water to 4.5. After the adjustment is completed, stir the fabric for 20 minutes. Take it out after completion;

[0043] 3) Dehydration of the fabric, the fabric fished out in...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a desizing treatment method for cotton-polyester blended fabrics, each part by weight is 1g, comprising the following steps: preparation of desizing liquid, pretreatment of fabrics, dehydration of fabrics, desizing treatment of fabrics, steaming treatment, Washing treatment and drying treatment; the desizing solution of the present invention is used to desizing the cotton-polyester blended fabric, the desizing rate is high, and the obtained fabric has high gross effect and mechanical properties, which is beneficial to the subsequent printing and dyeing process. The quality of subsequent printing and dyeing is guaranteed; and the hand feeling of the fabric is improved due to the effective removal of the size.

Description

technical field [0001] The invention relates to a desizing treatment method for cotton-polyester blended fabrics. Background technique [0002] In the textile dyeing and finishing process, the fabric with yarn as the warp must be sizing before weaving to improve the warp. [0003] The strength, abrasion resistance and smoothness of the yarn can be improved, thereby reducing warp yarn breakage and ensuring the smooth progress of weaving. The sizing materials used for warp yarn sizing include natural sizing materials such as starch and wild starch, chemical sizing materials such as polyvinyl alcohol (PVA), polyacrylic acid (PAA), and cellulose preparations such as carboxymethyl cellulose (CMC). Other ingredients such as preservatives, softeners, hygroscopic agents, wear-reducing agents, etc. are also added to the sizing solution. The warp sizing rate is related to fiber quality, yarn count, density, etc. For fabrics with fine yarn count and high density, the warp sizing rate...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): D06L1/14D06L1/16
CPCD06L1/14D06L1/16
Inventor 付宏杰孙青锋李洁赵晓华