Metal oil dirt cleaning agent and preparation method thereof
A technology for metal oil stains and cleaning agents, applied in the field of cleaning agents, can solve the problems of no anti-rust function, environmental hazards, time-consuming and labor-intensive, etc., and achieve the effects of protecting the metal surface, delaying corrosion, and avoiding redeposition.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0024] A preparation method of a metal oil stain cleaning agent, comprising the steps of:
[0025] According to the number of parts by mass, take 15~18 parts of metal oil stain cleaning agent A, 5~8 parts of metal oil stain cleaning agent B, 10~12 parts of metal oil stain cleaning agent C, 2~3 parts of isothiazolinone, 30~40 parts Deionized water is mixed to obtain metal oil stain cleaning agent.
Embodiment 1
[0027] Auxiliary A for metal oil stain cleaning agent: Take cornstarch, ethylene glycol, and dodecyl alcohol, mix them evenly in a mass ratio of 1:4:1, pass in steam, heat up to 100°C and keep for 1 hour to obtain a mixture, calculated in parts by mass , take 15 parts of the mixture, 2 parts of sodium hydroxide, 1 part of sodium dodecylbenzene sulfonate, 10 parts of ethylene glycol, 3 parts of hydrogen peroxide, and 1 part of sodium borohydride, mix them, heat up to 110 ° C for 1 h, and distill under reduced pressure , to obtain the vacuum distillate, in parts by mass, get 100 parts of deionized water, 2 parts of fatty alcohol polyoxyethylene ether sodium sulfate, 4 parts of fatty alcohol polyoxyethylene ether, 15 parts of vacuum distillate, and heat up to 45 Stir and mix for 30 minutes at ℃ to obtain a stirred mixture. Take the stirred mixture and add urea and alkanolamide in a mass ratio of 10:2:1, and keep at 65°C for 40 minutes to obtain metal oil stain cleaning agent A.
...
Embodiment 2
[0035] Auxiliary A for metal oil stain cleaning agent: Take cornstarch, ethylene glycol, and dodecyl alcohol, mix them evenly in a mass ratio of 1:4:1, pass in steam, raise the temperature to 105°C and keep for 2 hours to obtain a mixture, calculated in parts by mass , take 20 parts of the mixture, 3 parts of sodium hydroxide, 2 parts of sodium dodecylbenzenesulfonate, 12 parts of ethylene glycol, 4 parts of hydrogen peroxide, and 2 parts of sodium borohydride, mix them, heat up to 120 ° C for 2 hours, and distill under reduced pressure , to obtain the vacuum distillate, in parts by mass, get 100 parts of deionized water, 3 parts of fatty alcohol polyoxyethylene ether sodium sulfate, 5 parts of fatty alcohol polyoxyethylene ether, 20 parts of vacuum distillate, and heat up to 50 Stir and mix for 40 minutes at ℃ to obtain a stirred mixture. Take the stirred mixture and add urea and alkanolamide at a mass ratio of 10:2:1, and keep at 70°C for 50 minutes to obtain metal oil stain ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com