A sludge dehydration and conditioning agent technology, which is applied in the direction of water/sludge/sewage treatment, sludge treatment, chemical instruments and methods, etc., can solve problems such as inability to utilize resources, improve the efficiency of subsequent resource utilization, reduce Incremental issues, the effect of increasing the scope of application
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Mix 30 parts of fly ash, 20 parts of waste wood chips, 10 parts of diatomaceous earth, 10 parts of magnesium oxide and 10 parts of bauxite to make sludge conditioner A. Add PAM solution to the sludge with a moisture content of 99.2%, the addition amount is 1 mg / g DS relative to the absolute dry sludge, after the stock transfer treatment, add conditioner A therein, the addition amount is 0.05 g / g DS (relative to dry sludge), after stirring for 15 minutes, put the sludge into a high-pressure diaphragm filter press for dehydration, and the moisture content of the dehydrated sludge reaches 55.8%.
Embodiment 2
[0024] Fully mix 40 parts of fly ash, 10 parts of waste wood chips, 5 parts of diatomaceous earth, 5 parts of magnesium oxide and 20 parts of bauxite to prepare sludge conditioner A. Add PAM emulsion to the sludge with a water content of 98.1%, the addition amount is 3mg / g DS (relative to absolute dry sludge), after being treated by ordinary belt machine, add conditioner A to it, the addition amount is 0.1g / g gDS (compared to absolute dry sludge), after mixing evenly, the sludge is sent to a high-pressure belt machine for dehydration, and the moisture content of the dehydrated sludge reaches 57.3%.
Embodiment 3
[0026] Fully mix 40 parts of fly ash, 20 parts of waste wood chips, 5 parts of diatomaceous earth, 5 parts of magnesium oxide and 20 parts of bauxite to prepare sludge conditioner A. Add chitosan solution to the sludge with a water content of 97.6%, the addition amount is 2mg / gDS (relative to the absolute dry sludge), after being treated by the screw stacker, add conditioner A to it, the addition amount is 0.08g / gDS (relative to absolute dry sludge), after mixing evenly, the sludge is sent to a high-pressure belt machine for dehydration, and the moisture content of the dehydrated sludge reaches 52.7%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com