A technology of water-based coatings and compositions, applied in the direction of corona discharge devices, conductive coatings, polyurea/polyurethane coatings, etc., can solve the uneven distribution of coating surface resistance, the inability to maintain a uniform dispersion state, and affect the performance of conductive elastomer rolls etc., to achieve good storage stability, simple and feasible preparation method, and good performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0124] 5 parts by weight of conductive carbon black (trade name: Ketjenblack EC-300J; Akzo Nobel Company) as the first conductive filler, 8 parts by weight of acicular conductive titanium dioxide (trade name: TIPAQUE FT-3000; Ishihara Sangyo Co., Ltd. ) as the second conductive filler, 5 parts by weight of porous carbon microspheres (trade name: JCAC-1800; Nanjing Jicang Nano Technology Co., Ltd.) mixed as the third conductive filler, stirred and dispersed evenly for 0.5 hour, the conductive filler mixture was obtained ;
[0125] Disperse the above-mentioned conductive filler mixture and 40 parts by weight of water-based polytetrafluoroethylene (trade name: PTFE emulsion D210C; Japan Daikin Industry Co., Ltd.) in water, stir and disperse evenly for 1 hour to prepare a mixed solution;
[0126] Subsequently, the mixed solution obtained above and 60 parts by weight of water-based polyether polyol (trade name: water-based polyether polyurethane dispersion ACURE T213; Shanghai Yuan...
Embodiment 2
[0130] Except that the first conductive filler is a hollow carbon sphere (trade name: JCHCS-99-550; Nanjing Jicang Nano Technology Co., Ltd.) of 5 parts by weight, and the solid content in the water-based coating composition obtained is 12wt%, all the other according to the The same method as in Example 1 was used to obtain a developing roller.
Embodiment 3
[0132]Except that the second conductive filler and the third conductive filler were not added, and the solid content in the obtained water-based coating composition was 8 wt %, the developing roller was obtained by the same method as in Example 1.
PUM
| Property | Measurement | Unit |
|---|---|---|
| size | aaaaa | aaaaa |
| length | aaaaa | aaaaa |
| particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 