Embodiment 1
[0016] A filling gel used for fixing the internal battery of the power bank, consisting of the following components:
[0017] Base material: 100 parts of hydroxypolydimethylsiloxane; 60 parts of nano-scale calcium carbonate powder, 5 parts of zinc oxide;
[0018] Color masterbatch: one of cadmium red, cadmium yellow, titanium dioxide, carbon black, iron oxide red or iron oxide yellow;
[0019] Crosslinking agent: 1 part of methyltrimethoxysilane, 1 part of tetramethoxysilane, 1 part of vinyltriethoxysilane;
[0020] Coupling agent: 1 part of aminopropyltriethoxysilane;
[0021] Catalyst: 1 part of anilinomethyltriethoxysilane, 1 part of diethylaminomethyltriethoxysilane.
[0022] Further, preferably, the components also include a foaming agent, and the foaming agent is calcium carbonate.
[0023] Further, preferably, the components further include a heat dissipation agent, and the heat dissipation agent is an alumina heat conduction agent.
Embodiment 2
[0025] A filling gel used for fixing the internal battery of the power bank, consisting of the following components:
[0026] Base material: 100 parts of hydroxypolydimethylsiloxane; 60 parts of nano-scale calcium carbonate powder, 5 parts of zinc oxide;
[0027] Color masterbatch: one of cadmium red, cadmium yellow, titanium dioxide, carbon black, iron oxide red or iron oxide yellow;
[0028] Crosslinking agent: 1 part of methyltrimethoxysilane, 1 part of tetramethoxysilane, 1 part of vinyltriethoxysilane;
[0029] Coupling agent: 1 part of aminopropyltriethoxysilane;
[0030] Catalyst: 1 part of anilinomethyltriethoxysilane, 1 part of diethylaminomethyltriethoxysilane.
[0031] Further, preferably, the components also include a foaming agent, and the foaming agent is a combination of magnesium carbonate and sodium bicarbonate in any proportion.
[0032] Further, preferably, the components further include a cooling agent, and the cooling agent is one or a combination of si...
Embodiment 3
[0034] A filling gel used for fixing the internal battery of the power bank, consisting of the following components:
[0035] Base material: 100-120 parts of hydroxyl polydimethylsiloxane; 60-80 parts of nano-scale calcium carbonate powder, 5-10 parts of zinc oxide;
[0036] Color masterbatch: one of cadmium red, cadmium yellow, titanium dioxide, carbon black, iron oxide red or iron oxide yellow;
[0037] Crosslinking agent: 8 parts of methyltrimethoxysilane, 8 parts of tetramethoxysilane, 8 parts of vinyltriethoxysilane;
[0038] Coupling agent: 1 part of aminopropyltriethoxysilane;
[0039] Catalyst: 8 parts of anilinomethyltriethoxysilane and 6 parts of diethylaminomethyltriethoxysilane.
[0040] Further, preferably, the components also include a foaming agent, and the foaming agent is magnesium carbonate.
[0041] Further, preferably, the components further include a heat dissipation agent, and the heat dissipation agent is a combination of alumina heat conduction agent...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com