Multi-metal cassiterite sulfurizing tail concentrating method
A beneficiation method and sulfide ore technology, applied in chemical instruments and methods, flotation, wet separation, etc., can solve problems such as poor separation index, many valuable element components, and low grade, so as to ensure recovery rate and improve Effect of Recovery and Grade
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] Embodiment 1: Treatment of a cassiterite polymetallic sulfide ore tailing in Guangxi containing 0.56% tin, 0.89% lead, 0.78% antimony and 1.54% zinc. use as figure 1 Shown technological process, concrete technological parameter is:
[0021] ①Tail throwing: Use spiral concentrator equipment in parallel to recover materials from -2mm to +0.074mm from tailings with a concentration of 27%. Second sweep.
[0022] ②Pb-antimony-zinc mixed flotation: the dosage of butylamine black is 100 g / ton of raw ore, and the dosage of phenyl halide quaternary ammonium salt is 150 g / ton of raw ore; a process of roughing once and sweeping twice is adopted.
[0023] ③Lead antimony flotation: the dosage of ethylsulfurium helium is 100g / ton of raw ore, the dosage of zinc sulfate is 600g / ton of raw ore, the dosage of lime is 2500g / ton of raw ore, and the dosage of calcium humate is 500g / ton of raw ore. A process of rough selection, two scans, and four selections is adopted.
[0024] ④Zinc fl...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com