Embodiment 1
[0033] The transdermal patch described in this example is an adhesive matrix patch, consisting of a backing layer, a protective layer, and a drug-containing adhesive matrix (i.e., a drug reservoir). The materials used in each layer are as follows:
[0034] Backing layer: non-woven fabric
[0035] Protective layer: siliconized paper
[0036] Drug-containing adhesive skeleton: the formula is as follows (100 stickers):
[0037] Acrylic pressure sensitive adhesive 35g
[0038] Aconitin 2.5g
[0039] Azone 1.5g
[0040] Preparation process: Take aconitin, acrylate pressure-sensitive adhesive and Azone in the prescribed amount, add appropriate amount of ethyl acetate to dissolve, adjust to a suitable consistency, coat on the protective layer, and control the thickness of the coating. Dry at 70°C, cover with backing layer, and cut into proper shape and size.
Embodiment 2
[0042] The transdermal patch described in this example is an adhesive matrix patch, consisting of a backing layer, a protective layer, and a drug-containing adhesive matrix (i.e., a drug reservoir). The materials used in each layer are as follows:
[0043] Backing layer: non-woven fabric
[0044] Protective layer: polyester film
[0045] Drug-containing adhesive skeleton: the formula is as follows (100 stickers):
[0046] Polyacrylic resin pressure sensitive adhesive 30g
[0047] Aconitine 2g
[0048] Oleic acid 2g
[0049] The formula of polyacrylic resin pressure sensitive adhesive is:
[0050] Polyacrylic resin IV 20g
[0051] Succinic acid 1g
[0052] Dibutyl phthalate 10g
[0053] Acetone 80ml
[0054] Preparation Process:
[0055] 1. Preparation of polyacrylic resin pressure-sensitive adhesive: Dissolve the amount of succinic acid in acetone, then add polyacrylic acid resin and stir to dissolve, and finally add dibutyl phthalate and continue stirring for 20 minute...
Embodiment 3
[0058] The transdermal patch described in this example is an adhesive layer rate-limiting patch, which consists of a backing layer, a protective layer, a drug-containing adhesive skeleton (i.e. drug storage), and a four-layer structure of the adhesive layer. The materials are as follows:
[0059] Backing layer: polyester film
[0060] Protective layer: PTFE film
[0061] Adhesive layer: blank silicone pressure sensitive adhesive
[0062] Drug-containing viscose skeleton: the formula is as follows (100 stickers):
[0063] Silicone pressure sensitive adhesive 30g
[0064] Aconitine 1.0g
[0065] Azone 1.5g
[0066] Preparation Process:
[0067] 1. Preparation of drug-containing skeleton layer: Dissolve silicone pressure-sensitive adhesive, aconitin and Azone in an appropriate amount of ethyl acetate, adjust to a suitable consistency, and coat on the backing layer to control the coating thickness. Dry at 70°C.
[0068] 2. Preparation of adhesive layer: apply blank silicon...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com