Dry-film abyssal fish collagen peptide facial mask and preparation method thereof
A deep-sea fish skin and collagen peptide technology, applied in the field of chemistry, can solve the problems of environmental pollution, resource waste, discarding, etc., and achieve the effects of convenient use, convenient operation, and increased added value.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The following ingredients involved are by weight ratio,
[0019] (1) 5 parts of deep-sea fish skin collagen polypeptide, 2 parts of trehalose, 0.5 part of inulin and 0.2 part of starch were dissolved in deionized water, stirred evenly at 30°C, and set aside;
[0020] (2) Put 5 parts of sodium carboxymethylcellulose in a container, add deionized water, heat to 50°C and stir evenly, then slowly add the result of step (1), stir for 25 minutes, add rose hydrosol after cooling 1 part, 5 parts of sorbitol, continue to stir for 30 minutes;
[0021] (3) Pour the product obtained in step (2) into a mold to form it, and dry it at 60°C to obtain the finished product.
Embodiment 2
[0023] The following ingredients involved are by weight ratio,
[0024] (1) Dissolve 1 part of deep-sea fish skin collagen polypeptide, 1 part of trehalose, 1 part of inulin and 0.1 part of starch in deionized water, stir evenly at 40°C, and set aside;
[0025] (2) Put 10 parts of sodium carboxymethylcellulose in a container, add deionized water, heat to 60°C and stir evenly, then slowly add the result of step (1), stir for 20 minutes, add rose hydrosol after cooling 1.5 parts, 5 parts of glycerin, continue to stir for 25 minutes;
[0026] (3) Pour the product obtained in step (2) into a mold to form it, and dry it at 60°C to obtain the finished product.
Embodiment 3
[0028] The following ingredients involved are by weight ratio,
[0029] (1) Dissolve 10 parts of deep-sea fish skin collagen polypeptide, 1.5 parts of trehalose, 1 part of inulin and 1 part of starch in deionized water, stir evenly at 40°C, and set aside;
[0030] (2) Put 2 parts of sodium carboxymethylcellulose in a container, add deionized water, heat to 50°C and stir evenly, then slowly add the result of step (1), stir for 25 minutes, add rose hydrosol after cooling 2 parts, 8 parts of sorbitol, continue stirring for 20 minutes;
[0031] (3) Pour the product obtained in step (2) into a mold to form it, and dry it at 60°C to obtain the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com