Micro-emulsion ink cleaning agent and preparation method thereof
A cleaning agent and microemulsion technology, which is applied in the field of microemulsion ink cleaning agent and its preparation, can solve the problems of only cleaning ink rollers, reducing the proportion of organic solvents, and narrowing the scope of cleaning objects, and achieves low production cost and cleaning effect. Good, non-polluting effect to the environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] At room temperature, first mix 2g fatty alcohol polyoxyethylene sodium sulfate, 3g fatty alcohol polyoxyethylene ether (addition number is 9), 2g nonylphenol polyoxyethylene ether, 1g sodium dodecylbenzenesulfonate, 2g Alkanolamide, 2g of triethanolamine and 2g of penetrant fatty alcohol polyoxyethylene ether were added to 73g of pure water and stirred, dissolved, and prepared into a solution, and then under stirring conditions, 5g of n-butyl acetate was added for emulsification, stirred for 20min, and waited After the emulsion is stable, continue to add 8 g of ethylene glycol ether, and stir for 30 min to prepare 100 g of microemulsion ink cleaning agent.
Embodiment 2
[0021] At room temperature, first mix 1g potassium perfluorobutanesulfonate, 3g fatty alcohol polyoxyethylene ether (addition number is 15), 2g octylphenol polyoxyethylene ether, 2g sodium hexadecylbenzenesulfonate, 3g Hydroxyethylethylenediamine and 3g of fatty alcohol polyoxyethylene ether were added into 71g of pure water and stirred, dissolved, and prepared into a solution. Then, under stirring conditions, 3g of amyl acetate was added for emulsification, and stirred for 20 minutes. After the emulsion was stable, Continue to add 12g of propylene glycol methyl ether and stir for 30min to prepare a microemulsion ink cleaning agent.
Embodiment 3
[0023] At room temperature, first mix 2g fatty alcohol polyoxyethylene ether ammonium sulfate, 2g fatty alcohol polyoxyethylene ether (addition number is 10), 2g octylphenol polyoxyethylene ether, 1g dodecylbenzenesulfonic acid, 2g Add alkyl alcohol amide, 2g monoethanolamine and 2g fatty alcohol polyoxyethylene ether into 63g pure water and stir, dissolve, and prepare a solution, then add 8g propyl acetate to emulsify under stirring conditions, stir for 20min, and wait for the emulsion to be stable Afterwards, continue to add 18g propylene glycol butyl ether, stir 30min, make microemulsion ink cleaning agent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com