Reinforced formaldehyde-decomposed dope and preparation method thereof
A formaldehyde decomposition and enhancement technology, applied in the field of coatings and the preparation of the coatings, can solve the problems of unsuitability for popularization and application, human health hazards, unfavorable formaldehyde decomposition, etc., and achieves efficient removal of formaldehyde gas, good effect and low production cost. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] (1) Add 23 parts of water, 0.4 part of dispersant, 0.2 part of wetting agent, 0.2 part of defoamer and 1.5 part of film-forming aid into the mixing container in sequence, mix and stir evenly.
[0040] (2) Slowly add 10 parts of diatomaceous earth to the above-mentioned uniformly stirred mixture, and stir for 15 minutes at a speed of 2200 r / min to prepare a hydrocolloid slurry.
[0041] (3) Under low-speed stirring conditions, slowly add 29 parts of pigments and fillers to the above-mentioned water-based colloid slurry at the same time, increase the speed again after the addition, and stir for 30 minutes at a speed of 1500r / min; the low-speed stirring used in this step The speed is 500-700 r / min, preferably 600 r / min in this embodiment. The pigments and fillers used in the present invention are conventional pigments and fillers, including titanium dioxide, talc and kaolin. The pigments and fillers in this embodiment are selected from titanium dioxide, talc and kaolin. ...
Embodiment 2
[0047] Compared with Example 1, the difference of this example is that this example adds 5 parts of adsorbent, and changes the components of pigments and fillers, photocatalyst, water, and emulsion. That is, 5 parts of sepiolite are added in this embodiment; the pigment and filler are changed to 24 parts, diatomaceous earth is changed to 8 parts, water is changed to 24 parts, and pure acrylate emulsion is changed to 30 parts.
[0048] According to the indicators in GB / T 9756-2009 "Synthetic Resin Emulsion Interior Wall Coatings", the performance of the coating is tested. According to the test results, it shows that the conventional performance indicators of the coating meet the requirements of the national standard.
[0049] The product prepared according to this embodiment was subjected to a formaldehyde purification experiment according to the method described in the national building materials industry standard "Purification Performance of Wall Coating Materials with Air Pur...
Embodiment 3
[0051] Compared with Example 2, the difference of this example is that the photocatalyst is the modified diatomite-loaded nano-TiO from Meishidun Powder Materials Co., Ltd., Linjiang City, Jilin Province. 2 composite material. The difference of this embodiment is that the components of pigments and fillers, photocatalyst, water and emulsion are different; this embodiment uses 22 parts of pigments and fillers, 10 parts of photocatalyst, 21 parts of water and 33 parts of emulsion.
[0052] According to the indicators in GB / T 9756-2009 "Synthetic Resin Emulsion Interior Wall Coatings", the performance of the coating is tested. According to the test results, it shows that the conventional performance indicators of the coating meet the requirements of the national standard.
[0053] The product prepared according to this embodiment was subjected to a formaldehyde purification experiment according to the method described in the national building materials industry standard "Purifica...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com