Moisturecured one-component polyurethane paint and preparation method thereof

A polyurethane coating, one-component technology, used in polyurea/polyurethane coatings, coatings, etc., can solve the problems of cumbersome procedures, high tensile strength, reduced storage stability, etc., and achieve good physical and mechanical properties and system viscosity changes. Small, the effect of improving storage stability

Active Publication Date: 2012-09-19
苏州中材非金属矿工业设计研究院有限公司 +1
View PDF3 Cites 31 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] However, moisture-curing one-component polyurethane coatings also have some shortcomings: ①The coating is cured by slow reaction by absorbing moisture, so it is greatly affected by air humidity and the curing time is longer. Adding a drier can improve the coating The drying speed of the film, but it will reduce the storage stability; ②Due to the carbon dioxide generated by moisture curing, it cannot be thickly coated, and multiple layers of coating and scraping are required during construction. The procedure is cumbersome, which may affect the construction period; ③The addition of powder can reduce costs, but It will increase the viscosity of the system, and it is necessary to add a diluent solvent, making the product not environmentally friendly
However, in order to ensure the stability of the mechanical properties of the coating film after curing, the amount of water added must be strictly controlled. If the moisture content is too low, the curing of the coating film will be slow. As the water content increases, the mechanical properties increase accordingly. When the water content is in a certain range, the tensile strength is the highest; when the water content is too much, the mechanical properties decrease.
These have caused many difficulties to the application of water-curable polyurethane waterproof coatings, which are also the shortcomings of water-curable polyurethane waterproof coatings.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Moisturecured one-component polyurethane paint and preparation method thereof
  • Moisturecured one-component polyurethane paint and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0030] This embodiment provides a moisture-curing one-component polyurethane coating and a preparation method thereof.

[0031] In terms of parts by weight, the raw materials of moisture-curing one-component polyurethane coatings are: 18 parts of diphenylmethane diisocyanate MI-50 (BASF), polyether polyol (DL-2000, Shandong Bluestar Dongda Chemical Co., Ltd. company) 35 parts, propylene carbonate 10 parts, silane coupling agent modified calcined kaolin 35 parts, oxazolidine curing agent (FT-103, Zhangjiagang Feite Company) 1 part, cyclodextrin-coated organic bismuth complex 0.5 parts of substance (Shanghai Hemu Chemical Co., Ltd.), 0.3 parts of defoamer (BYK-378) and 0.2 parts of p-toluenesulfonyl isocyanate (Sinopharm Chemical Reagent Co., Ltd.).

[0032] The preparation method of moisture curing one-component polyurethane coating is as follows:

[0033]Step 1: Add DL-2000, propylene carbonate and silane coupling agent modified calcined kaolin into the closed reaction kettle...

Embodiment 2

[0037] This embodiment provides a moisture-curing one-component polyurethane coating and a preparation method thereof.

[0038] In terms of parts by weight, the raw materials of moisture-curing one-component polyurethane coatings are: 16 parts of diphenylmethane diisocyanate MI-50 (BASF), polyether polyol (DL-2000, Shandong Bluestar Dongda Chemical Co., Ltd. Company) 30 parts, polyether polyol (EP-330N) 10 parts, propylene carbonate 10 parts, silane coupling agent modified talcum powder 30 parts, oxazolidine curing agent (FT-103, Zhangjiagang Feite Company) 2 1 part, cyclodextrin-coated organic bismuth complex (Shanghai Hemu Chemical Co., Ltd.), 0.3 part of defoamer (BYK-378) and p-toluenesulfonyl isocyanate (Sinopharm Chemical Reagent Co., Ltd.) 0.5 servings.

[0039] The preparation method of moisture curing one-component polyurethane coating is as follows:

[0040] Step 1: Add DL-2000, EP-330N, propylene carbonate and silane coupling agent modified talcum powder into the ...

Embodiment 3

[0044] This embodiment provides a moisture-curing one-component polyurethane coating, which is prepared by the same method as in Embodiment 1. In parts by weight, the raw material composition of the moisture-curing one-component polyurethane coating is as follows:

[0045] 12 parts of IPDI (Bayer company), 30 parts of polyether polyol (DL-2000, Shandong Bluestar Dongda Chemical Co., Ltd.), 5 parts of polyether polyol (DL-3000), 10 parts of propylene carbonate, silane di 40 parts of talcum powder modified by joint agent, 2 parts of oxazolidine curing agent (FT-103, Zhangjiagang Feite Company), 1 part of organic bismuth complex coated with cyclodextrin (Shanghai Hemu Chemical Co., Ltd.), disinfectant 0.5 parts of foaming agent (BYK-378) and 0.5 parts of p-toluenesulfonyl isocyanate (Sinopharm Chemical Reagent Co., Ltd.).

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
Functional group degreeaaaaaaaaaa
Login to view more

Abstract

The invention relates to moisturecured one-component polyurethane paint and a preparation method thereof. The polyurethane paint comprises the following raw materials in percentage by weight: 10%-20% of polyisocyanate monomer, 20%-40% of polyether polylol, 5%-15% of plasticizer, 30%-50% of modified mineral powder, 1%-5% of latent curing agent, 0.1%-2% of environment-friendly catalyst covered with cyclodextrin, 0.1%-1% of defoamer and 0.1%-1% of mono-isocyanate compound, wherein the modified mineral powder is mineral powder of which the surface is covered with a covered agent by a chemical covering method; and the environment-friendly catalyst covered with the cyclodextrin is in a nanometer cavity of the cyclodextrin, and the cyclodextrin is unmodified cyclodextrin or modified cyclodextrin or the composition of the unmodified cyclodextrin and the modified cyclodextrin. The moisturecured polyurethane paint disclosed by the invention solves the problem in storage stability of a one-component polyurethane product, and the storage life of the moisturecured polyurethane paint can exceed one year.

Description

technical field [0001] The invention relates to a protective coating, in particular to a protective coating used in the construction field and a preparation method thereof. Specifically, the invention relates to a moisture-curing one-component polyurethane coating and a preparation method thereof. Background technique [0002] Moisture-curing one-component polyurethane coatings are prepolymers containing isocyanate (-NCO) end groups, suitable for construction in humid environments, can react with moisture, and further cross-link and cure to form highly elastic, durable non-joint Seam waterproof coating. The coating film contains a large number of urea bonds and urethane bonds. Due to the effect of hydrogen bonds, the coating film has excellent adhesion, wear resistance, oil resistance, acid and alkali resistance, impact resistance, and good electrical insulation. The film-forming substances of such coatings are mostly prepared by the addition reaction of macromolecular pol...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D175/08C09D7/12C08G18/76C08G18/71C08G18/48C08G18/08
Inventor 沈春林金伟康康杰分陈鸿根褚建军王玉峰杨炳元杨乃浩
Owner 苏州中材非金属矿工业设计研究院有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products