Technology for producing phosphate from pyrophosphate
A pyrophosphate and phosphate technology, which is applied in the field of phosphorus chemical industry, can solve the problems of increasing processing procedures, increasing equipment investment, hindering the reuse, application and promotion of phosphorus-containing wastes, and achieving a concise process route and product quality. Enhancement, good environmental protection effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] (1) Take crude sodium pyrophosphate with a sodium pyrophosphate content of more than 81%, add water to wash and perform desalination treatment, and the content of sodium chloride in the obtained desalted crude sodium pyrophosphate is lower than 0.8%;
[0034] (2) Take 1000g of the obtained desalted crude sodium pyrophosphate, add 2500g of water, heat to dissolve and filter to remove the insoluble solid;
[0035] (3) Heat up the obtained sodium pyrophosphate solution for hydrolysis reaction. The reaction temperature is 130-150°C, the reaction pressure is 0.4MP, and the reaction time is 3h. The depolymerized sodium phosphate solution is obtained. The pH value of the obtained sodium phosphate solution is 8.7;
[0036] (4) Add 10g of sodium sulfide to the obtained sodium phosphate solution, stir, set aside for precipitation and filter to obtain the product sodium phosphate solution. 25ppm.
[0037] further
[0038] (5) Add 700g of 85% phosphoric acid to the obtained prod...
Embodiment 2
[0040] (1) Take the crude sodium pyrophosphate with a sodium pyrophosphate content of more than 81% and grind it to 60 meshes, add water to wash the crushed crude sodium pyrophosphate and perform desalination treatment, so that the content of sodium chloride in the desalted crude sodium pyrophosphate less than 0.6%;
[0041] (2) Take 1000g of the obtained desalted crude sodium pyrophosphate, add 2500g of water, heat to dissolve and filter to remove the insoluble solid;
[0042] (3) Add 60g of sodium carbonate to the obtained sodium pyrophosphate solution, stir evenly and heat up to carry out the hydrolysis reaction, the reaction temperature is controlled at 125-130°C, the reaction pressure is about 0.25MPa, and the reaction time is 4h to obtain depolymerized Sodium phosphate solution, the pH value of gained sodium phosphate solution is 10;
[0043] (4) Add 85% phosphoric acid to the obtained sodium phosphate solution to adjust the pH of the solution to 7, stir, set aside for pr...
Embodiment 3
[0047] (1) Take the crude sodium pyrophosphate with a sodium pyrophosphate content of more than 81% and grind it to 60 meshes, add water to wash the crushed crude sodium pyrophosphate and perform desalination treatment, so that the content of sodium chloride in the desalted crude sodium pyrophosphate less than 0.6%;
[0048] (2) Take 1000g of the obtained desalted crude sodium pyrophosphate, add 2500g of water, heat to dissolve and filter to remove the insoluble solid;
[0049] (3) Add 30% sodium hydroxide to the obtained sodium pyrophosphate solution to adjust the pH of the solution to 12.0, stir evenly and heat up to carry out the hydrolysis reaction. The reaction temperature is controlled at 170-200°C, the reaction pressure is about 0.8MPa, and the reaction time is For 1h, the sodium phosphate solution after depolymerization was obtained, and the pH value of the gained sodium phosphate solution was 10.0;
[0050] (4) Add 5g of phosphorus pentasulfide to the obtained sodium...