A manufacturing method and door panel technology, which is applied in the field of building material processing, can solve the problems of insufficient molding, sound insulation of veneer, moisture resistance, insufficient rigidity, and shortage, etc., and achieve good impact resistance and aging resistance, good sound and heat absorption effects, The effect of simple production process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] The manufacture method of door panel of the present invention comprises the steps:
[0023] A. Saw off the bent edge of the bumper of scrapped cars, keep the plate-shaped part of 500mm*1000mm, prepare two plywood pieces of 1000*2000mm, coat one side of the two plywood boards with urea-formaldehyde resin respectively, and then coat them with glue Lay two treated scrapped automobile bumper panels side by side on the surface of the three-ply board, and then press the surface of another three-ply board coated with glue on the scrapped automobile bumper board, and stack it well to obtain a basic composite board; The combined composite board is sent to the hot press for hot pressing and shaping. The temperature of the hot press is set at 150°C, the pressure is 10Mp, and the hot pressing time is 10min. The formed composite board is then sent to the cold press for cold pressing. Finalize the shape, the temperature of the cold press is 20°C, the pressure is 5Mp, the cold pressin...
Embodiment 2
[0029] A. Saw off the bent edge of the scrapped automobile bumper, keep the plate-shaped part of 500mm*1000mm, prepare two five-plywood boards of 1000*2000mm, and coat one side of the two five-plywood boards with phenolic resin respectively. Lay two treated scrapped automobile bumper panels side by side on the surface of the five-plywood with glue, and then press the surface of another five-plywood coated with glue on the scrapped automobile bumper panel, and stack them well to obtain a basic composite board; the laminated composite board is sent to a hot press for hot pressing and shaping. The temperature of the hot press is set to 170°C, the pressure is 15Mp, and the hot pressing time is 5min. The formed composite board is then sent to the cold press In the process, the cold pressing is finalized, the temperature of the cold pressing machine is 10°C, the pressure is 8Mp, and the cold pressing time is 15min, and the composite wood-based panel is obtained;
[0030] B. Splicing...