Water soluble nacre powder chelation technology
A technology of nacre and nacre powder, which is applied in the fields of food science, food preparation, cosmetic preparations, etc., can solve the problems of high cost of nacre powder, environmental pollution, and unsuitability for promotion, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] The invention provides a kind of water-soluble nacre powder chelation process, comprises the following steps:
[0030] 1) Liquid-solid phase reaction: take the pretreated coarse nacre powder and place it in a container, where the container is an open container, add a gluconic acid solution with a mass fraction of 45%, and keep the reaction temperature at 85°C until there is no CO 2 Generate gas, stop the reaction, filter and dry to obtain organic acid nacre powder; using organic acid available in the food industry, that is, gluconic acid solution, can effectively avoid the destruction of the nutritional components of nacre powder by using inorganic acids such as hydrochloric acid and nitric acid , add gluconic acid solution to coarse nacre powder until CO is free 2 Gas generation stops the reaction, which can ensure the complete reaction of the coarse nacre powder; if the reaction temperature is too low, the reaction rate is too low, and the reaction temperature is too ...
Embodiment 2
[0035] 1) Liquid-solid phase reaction: take the pretreated coarse nacre powder and place it in a container, where the container is an open container, add a gluconic acid solution with a mass fraction of 50%, and keep the reaction temperature at 90°C until there is no CO 2 Generate gas, stop the reaction, filter and dry to obtain organic acid nacre powder; using organic acid available in the food industry, that is, gluconic acid solution, can effectively avoid the destruction of the nutritional components of nacre powder by using inorganic acids such as hydrochloric acid and nitric acid , add gluconic acid solution to coarse nacre powder until CO is free 2 Gas generation stops the reaction, which can ensure the complete reaction of the coarse nacre powder; if the reaction temperature is too low, the reaction rate is too low, and the reaction temperature is too high, the nutrients in the coarse nacre powder will be destroyed. The reaction temperature is 90°C, which can ensure Th...
Embodiment 3
[0040] 1) Liquid-solid phase reaction: take the pretreated coarse nacre powder and place it in a container, where the container is an open container, add a gluconic acid solution with a mass fraction of 55%, and keep the reaction temperature at 95°C until there is no CO 2Generate gas, stop the reaction, filter and dry to obtain organic acid nacre powder; using organic acid available in the food industry, that is, gluconic acid solution, can effectively avoid the destruction of the nutritional components of nacre powder by using inorganic acids such as hydrochloric acid and nitric acid , add gluconic acid solution to coarse nacre powder until CO is free 2 Gas generation stops the reaction, which can ensure the complete reaction of the coarse nacre powder; if the reaction temperature is too low, the reaction rate is too low, and the reaction temperature is too high, the nutrients in the coarse nacre powder will be destroyed. The reaction temperature is 95°C, which can ensure The...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com