Production method of low-foam printing rubber roller printing ink cleaner
A technology of printing rubber roller and manufacturing method, applied in the direction of chemical paint/ink remover, coating, etc., can solve problems such as water waste, and achieve the effects of good stability, convenient use and good biodegradability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Raw material ratio (percentage by weight): 80% isopropanol, 5% limonene, 5% alkyl polyglycoside, 7% monobutyl polyether, 3% sodium laurylalanine.
Embodiment 2
[0023] Raw material ratio (percentage by weight): 70% isopropanol, 10% limonene, 7% alkyl polyglycoside, 8% monobutyl polyether and 5% sodium laurylalanine.
Embodiment 3
[0025] Raw material ratio (percentage by weight): 60% isopropanol, 15% limonene, 9% alkyl polyglycoside, 9% monobutyl polyether and 7% sodium laurylalanine.
[0026] The preparation steps are as follows: in a reaction vessel, sequentially add isopropanol, limonene, alkyl polyglycoside, monobutyl polyether and sodium dodecylalanine; react for 0.5-1 hour, and control the temperature at 10-40 After the reaction is completed, it is lowered to room temperature, and the material is discharged after passing the test. The finished product should be stored in a metal container.
[0027] Preferably, the reaction temperature is 20°C or 30°C.
[0028] Preferably, the reaction time is 1 hour.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com