[0020] 1) 10 parts of refined cotton powder, 5 parts of propylene oxide, 4 parts of chloroacetic acid, 50 parts of isopropanol, 100 parts of water, 30 parts of potassium hydroxide, mix the above materials, react at 50 degrees Celsius for 4 hours, and use acetone Precipitate, wash with alcohol solvent, and dry to obtain water-soluble hydroxyethyl carboxymethyl cellulose;
[0021] 2) Take 5 parts of hydroxyethyl carboxymethylcellulose obtained in step 1), add it to 80 parts of water, then add 2 parts of potassium carbonate, 1 part of sodium humate, 2 parts of acetic acid, 12 parts of sepiolite powder, 6 parts of 1 part of cross-linked rectorite, 8 parts of chitosan were stirred and dissolved at 30 degrees Celsius for 30 minutes, then 2 parts of defoamer 664, 1 part of hydrolyzed polymaleic anhydride (HPMA), 1 part of fatty acid polyoxyethylene ether were added to increase the temperature Continue to stir for 1 hour at 40 degrees Celsius, then add 2 parts of polydimethylsiloxane ...
Embodiment 2
[0023] 1) 10 parts of refined cotton powder, 15 parts of propylene oxide, 4 parts of chloroacetic acid, 50 parts of isopropanol, 100 parts of water, 30 parts of potassium hydroxide, mix the above materials, react at 50 degrees Celsius for 4 hours, and use acetone Precipitate, wash with alcohol solvent, and dry to obtain water-soluble hydroxyethyl carboxymethyl cellulose;
[0024] 2) Take 10 parts of hydroxyethyl carboxymethylcellulose obtained in step 1), add it to 95 parts of water, then add 8 parts of potassium carbonate, 3 parts of sodium humate, 5 parts of acetic acid, 15 parts of sepiolite powder, 8 parts of cross-linked rectorite, 12 parts of chitosan were stirred and dissolved at 30 degrees Celsius for 30 minutes, and then 5 parts of defoamer 664, 6 parts of hydrolyzed polymaleic anhydride (HPMA), and 6 parts of fatty acid polyoxyethylene ether were added to increase the temperature Continue to stir for 1 hour at 40 degrees Celsius, then add 3 parts of polydimethylsilox...
Embodiment 3
[0026] 1) 10 parts of refined cotton powder, 20 parts of propylene oxide, 4 parts of chloroacetic acid, 50 parts of isopropanol, 100 parts of water, 30 parts of potassium hydroxide, mix the above materials, react at 50 degrees Celsius for 4 hours, and use acetone Precipitate, wash with alcohol solvent, and dry to obtain water-soluble hydroxyethyl carboxymethyl cellulose;
[0027] 2) Take 15 parts of hydroxyethyl carboxymethylcellulose obtained in step 1), add it to 110 parts of water, then add 12 parts of potassium carbonate, 5 parts of sodium humate, 8 parts of acetic acid, 18 parts of sepiolite powder, 10 parts of cross-linked rectorite, 15 parts of chitosan were stirred and dissolved at 30 degrees Celsius for 30 minutes, and then 8 parts of defoamer 664, 10 parts of hydrolyzed polymaleic anhydride (HPMA), and 10 parts of fatty acid polyoxyethylene ether were added to increase the temperature Continue to stir for 1 hour at 40 degrees Celsius, then add 4 parts of polydimethyl...