Preparation method of automobile surface polishing agent
A technology for automobile surface and polishing agent, which is applied in the field of preparation of automobile surface polishing agent, can solve the problem that the wax film is difficult to ensure the uniformity and polishing of coating, and achieves the effects of low production cost, simple preparation process and good stability.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0023] 10. First weigh 1g of chloroplatinic acid and put it into a 100mL beaker, then measure 20mL of isopropanol and pour it into the beaker, stir evenly with a glass rod, so that chloroplatinic acid is completely dissolved in isopropanol, and prepare chloroplatinic acid-isopropyl alcohol Alcohol catalytic solution, spare; take a glass column with a diameter of 20mm and a length of 600mm, fill it with activated alumina, and then pass 500mLα-decene through the activated alumina glass at a rate of 40mL / h under nitrogen protection column to obtain pretreated colorless α-decene; add 20 g of pretreated α-decene to a magnetically stirred glass reactor, fill it with nitrogen, and move it into a water bath to raise the temperature to 65 ° C. Add 20g of hydrogen-containing silicone oil dropwise, control the dropping rate so that it will be dropped within 60min, then continue to heat up to 105°C, add dropwise 5mL of the chloroplatinic acid-isopropanol catalytic solution prepared above,...
example 2
[0026] 12. First weigh 1.5g of chloroplatinic acid and put it into a 100mL beaker, then pour 30mL of isopropanol into the beaker, stir evenly with a glass rod, and completely dissolve chloroplatinic acid in isopropanol to prepare chloroplatinic acid-isopropanol Propanol catalytic solution, spare; take a glass column with a diameter of 20mm and a length of 600mm, fill it with activated alumina, and then pass 550mLα-decene through activated alumina at a rate of 40mL / h under nitrogen protection Glass column to obtain pretreated colorless α-decene; add 23g of pretreated α-decene to the magnetic stirring glass reactor, and fill it with nitrogen, move it into a water bath and heat up to 68°C, Add 23g of hydrogen-containing silicone oil drop by drop, control the dropping speed so that it will be dropped within 65min, then continue to heat up to 108°C, add dropwise 7.5mL of the chloroplatinic acid-isopropanol catalytic solution prepared above, stir evenly with a glass rod and Continu...
example 3
[0029] 13. First weigh 2g of chloroplatinic acid into a 100mL beaker, then measure 40mL of isopropanol into the beaker, stir evenly with a glass rod, completely dissolve chloroplatinic acid in isopropanol, and prepare chloroplatinic acid-isopropyl alcohol Alcohol catalytic solution, spare; take a glass column with a diameter of 20mm and a length of 600mm, fill it with activated alumina, and then pass 600mLα-decene through the activated alumina glass at a rate of 40mL / h under nitrogen protection column to obtain pretreated colorless α-decene; add 25g of pretreated α-decene to a magnetically stirred glass reactor, fill it with nitrogen, move it into a water bath and raise the temperature to 75°C, gradually Add 25g of hydrogen-containing silicone oil dropwise, control the dropping rate so that it will be dropped within 70min, then continue to heat up to 110°C, add dropwise 10mL of the chloroplatinic acid-isopropanol catalytic solution prepared above, stir evenly with a glass rod ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com