Acid-resisting finishing method for viscose fabric

A technology of fabric and viscose, which is applied in fiber treatment, plant fiber, textiles and papermaking, etc. It can solve the problems of corrosion of work clothes, corrosion of employees, and low acid resistance, and achieves easy washing, resistance to strong acid erosion, prevention of wetting and penetration effect

Inactive Publication Date: 2016-06-22
HUZHOU HONGXIN SILK FACTORY
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

If the acid resistance of the work clothes is poor, when it is corroded by acid liquid, it will corrode the work clothes to a certain extent, and may seriously corrode the employees.
Viscose fabric has good air permeability and humidity control function, but its acid resistance is not high, which limits its application range

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0016] A method for acid-resistant finishing of viscose fabrics, which has the following steps: first add water to the finishing agent to prepare an impregnating solution, then put the fabric into the impregnating solution for padding, the excess rate is 45-70%, and finally wash it with water for 2-3 times, Finally, it can be dehydrated and dried; the finishing agent is composed of the following components in parts by weight: 20 parts of water, 6 parts of sodium polystyrene sulfonate, 5 parts of dimethyl terephthalate, 2 parts of ethylenediaminetetraacetic acid 4 parts of sodium, 1 part of acrylamide, 22 parts of butyl acetate, 5 parts of methylcyclosiloxane, 3 parts of didecyldimethyl ammonium chloride, 11 parts of isocyanate trimer, 4 parts of methyl hydrogen silicone oil , 4 parts of o-hydroxybenzoate, 4 parts of vinyl triethoxysilane, 1 part of fatty alcohol polyoxyethylene ether.

[0017] The fabric is soaked at 50-85°C for 20-30 minutes.

[0018] The drying temperature ...

Embodiment 2

[0021] A method for acid-resistant finishing of viscose fabrics, which has the following steps: firstly add water to the finishing agent to prepare an impregnating solution, then put the fabric into the impregnating solution for padding, the excess rate is 45-70%, and finally wash with water for 2-3 times, Finally, it can be dehydrated and dried; the finishing agent is composed of the following components in parts by weight: 50 parts of water, 9 parts of sodium polystyrene sulfonate, 6 parts of dimethyl terephthalate, ethylenediaminetetraacetic acid 7 parts of sodium, 6 parts of acrylamide, 25 parts of butyl acetate, 8 parts of methylcyclosiloxane, 7 parts of didecyldimethyl ammonium chloride, 16 parts of isocyanate trimer, 8 parts of methyl hydrogen silicone oil , 8 parts of o-hydroxybenzoate, 8 parts of vinyl triethoxysilane, 5 parts of fatty alcohol polyoxyethylene.

[0022] The fabric is soaked at 50-85°C for 20-30 minutes.

[0023] The drying temperature is 50-60° C., an...

Embodiment 3

[0026] A method for acid-resistant finishing of viscose fabrics, which has the following steps: firstly add water to the finishing agent to prepare an impregnating solution, then put the fabric into the impregnating solution for padding, the excess rate is 45-70%, and finally wash with water for 2-3 times, Finally, it can be dehydrated and dried; the finishing agent is composed of the following components in parts by weight: 30 parts of water, 7 parts of sodium polystyrene sulfonate, 5 parts of dimethyl terephthalate, 2 parts of ethylenediaminetetraacetic acid 5 parts of sodium, 5 parts of acrylamide, 24 parts of butyl acetate, 6 parts of methylcyclosiloxane, 5 parts of didecyldimethyl ammonium chloride, 14 parts of isocyanate trimer, 6 parts of methyl hydrogen silicone oil , 6 parts of o-hydroxybenzoate, 6 parts of vinyl triethoxysilane, 3 parts of fatty alcohol polyoxyethylene ether.

[0027] The fabric is soaked at 50-85°C for 20-30 minutes.

[0028] The drying temperature...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
elongation at breakaaaaaaaaaa
Login to View More

Abstract

The invention discloses an acid-resisting finishing method for viscose fabric. The method comprises the following steps: a finishing agent is mixed with water to be made into an impregnation liquid, fabric is put into the impregnation liquid for padding, the pick-up rate is 45%-70%, finally, the fabric is washed with water twice or three times, and the viscose fabric can be obtained after water removal and drying. The finishing agent comprises components in parts by weight as follows: 20-50 parts of water, 6-9 parts of sodium polystyrene sulfonate, 5-6 parts of dimethyl terephthalate, 4-7 parts of ethylenediamine tetracetic acid disodium salt, 1-6 parts of acrylamide, 22-25 parts of butyl acetate, 5-8 parts of dimethylcydosiloxane, 3-7 parts of didecyl dimethyl ammonium chloride, 11-16 parts of an isocyanate trimer, 4-8 parts of methyl hydrogen silicone oil, 4-8 parts of o-hydroxybenzoic ester, 4-8 parts of vinyltriethoxysilane and 1-5 parts of fatty alcohol-polyoxyethylene ether. With the adoption of the acid-resisting finishing method, the viscose fabric can be prevented from being wetted and permeated by an acid liquid, can resist corrosion of strong acid and has the advantages of being breathable, comfortable, soft, light, easy to wash and the like.

Description

technical field [0001] The invention belongs to the technical field of textiles, and in particular relates to an acid-resistant finishing method for viscose fabrics. technical background [0002] Viscose fabric is a fabric woven from viscose fiber, which is one of the earliest chemical fibers put into industrial production. Because of its good hygroscopicity, comfortable wearing and excellent spinnability, it is often blended and interwoven with cotton, wool or various synthetic fibers for various clothing and decorative textiles. Viscose fiber is a widely used chemical fiber. It is made of alkali cellulose by alkalization of natural cellulose, and then reacted with carbon disulfide to generate cellulose xanthate. The viscous solution obtained by dissolving in dilute lye is called viscose. Glue and viscose are made into viscose fiber through wet spinning and a series of post-processing procedures. Viscose fiber has good hygroscopicity, and the moisture regain is about 13% ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): D06M15/233D06M15/643D06M15/53D06M13/224D06M13/41D06M13/513D06M13/463D06M101/06
CPCD06M15/233D06M13/224D06M13/41D06M13/463D06M13/513D06M13/5135D06M15/53D06M15/643D06M2101/06D06M2200/50
Inventor 董根琴
Owner HUZHOU HONGXIN SILK FACTORY
Features
  • R&D
  • Intellectual Property
  • Life Sciences
  • Materials
  • Tech Scout
Why Patsnap Eureka
  • Unparalleled Data Quality
  • Higher Quality Content
  • 60% Fewer Hallucinations
Social media
Patsnap Eureka Blog
Learn More