An environment-friendly compound emulsifier for fuel oil
A composite emulsifier, environmentally friendly technology, used in fuel additives, fuel, petroleum industry and other directions, can solve the problems of incomplete combustion reaction, efficient combustion of fuel oil, environmental pollution, etc., and achieve easy recovery, efficient combustion, and wide application system. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] Environmentally friendly fuel compound emulsifier, prepared from basic components and modified components in an organic solvent at a mass ratio of 4:1, the basic components include 40 parts of styrene and methyl methacrylate, perfluorooctyl 2 parts of alkanesulfonic acid, 2 parts of butylbenzyl phthalate, 0.5 part of nonylphenol polyoxyethylene ether, 6 parts of methyl benzotriazole; modified components include sodium sulfomethyl humate 2 parts, 10 parts of Span 80, 10 parts of cobalt naphthenate, 5 parts of triisopropanolamine, 18 parts of phthalic anhydride, 10 parts of glycerol oleate, 4 parts of octadecanoic acid.
[0041] Prepare according to the following method: a. Add the organic solvent into the reaction kettle, heat up to 50-70°C, then mix the acrylate monomer and perfluorooctane sulfonic acid evenly, then slowly drop into the organic solvent, and control the feeding time After feeding, continue the heat preservation reaction for 2-4h, stop the reaction and co...
Embodiment 2
[0043] Environmentally friendly fuel compound emulsifier, prepared from basic components and modified components in an organic solvent at a mass ratio of 5:1, the basic components include 40 parts of styrene and methyl methacrylate, perfluorooctyl 5 parts of alkanesulfonic acid, 2 parts of butylbenzyl phthalate, 0.5 parts of nonylphenol polyoxyethylene ether, 6 parts of methyl benzotriazole; modified components include sodium sulfomethyl humate 3 parts, 12 parts of Span 80, 15 parts of cobalt naphthenate, 5 parts of triisopropanolamine, 20 parts of phthalic anhydride, 12 parts of glycerol oleate, 4 parts of octadecanoic acid.
[0044] Prepare according to the following method: a. Add the organic solvent into the reaction kettle, heat up to 50-70°C, then mix the acrylate monomer and perfluorooctane sulfonic acid evenly, then slowly drop into the organic solvent, and control the feeding time After feeding, continue the heat preservation reaction for 2-4h, stop the reaction and c...
Embodiment 3
[0046] Environmentally friendly fuel compound emulsifier, prepared from basic components and modified components in an organic solvent at a mass ratio of 5:1, the basic components include 50 parts of styrene and methyl methacrylate, perfluorooctyl 10 parts of alkanesulfonic acid, 3 parts of butylbenzyl phthalate, 1 part of nonylphenol polyoxyethylene ether, 8 parts of methyl benzotriazole; modified components include sodium sulfomethyl humate 8 parts, 15 parts of Span 80, 20 parts of cobalt naphthenate, 8 parts of triisopropanolamine, 25 parts of phthalic anhydride, 15 parts of glycerol oleate, 6 parts of octadecanoic acid.
[0047] Prepare according to the following method: a. Add the organic solvent into the reaction kettle, heat up to 50-70°C, then mix the acrylate monomer and perfluorooctane sulfonic acid evenly, then slowly drop into the organic solvent, and control the feeding time After feeding, continue the heat preservation reaction for 2-4h, stop the reaction and coo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com