Anticorrosive paint for door and preparation method thereof

A technology of anti-corrosion coatings and parts by weight, applied in anti-corrosion coatings, fire-retardant coatings, powder coatings, etc., can solve the problems of no insulation effect, high temperature resistance, general anti-corrosion performance, etc., and achieve good anti-corrosion effect and long coating life. , the effect of chemical stability

Inactive Publication Date: 2017-01-11
ANHUI KATA DOOR & WINDOW
View PDF4 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] At present, the anti-corrosion coating of the existing door has general anti-corrosion performance, and is not resistant to high temperature, has no insulation effect, and cannot maintain a long service life of the coating.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0019] An anti-corrosion coating for doors is made of the following materials in parts by weight: 35 parts of barium hydroxide, 20 parts of zinc oxide, 15 parts of aluminum naphthenate soap, 7 parts of barium chromate, 22 parts of ceramic micropowder, 9 parts of silicon carbide, 50 parts of phenolic epoxy resin, 3 parts of aluminum phosphate, 7 parts of polyvinyl butyral, 6 parts of butadiene resin film former, 4 parts of acrylic resin, 2 parts of mica, phytic acid ester 3 parts, 12 parts of chlorinated paraffin, 8 parts of toluenesulfonic acid, 6 parts of lithopone, 11 parts of biuret, 22 parts of polysiloxane, 8 parts of cooked tung oil and 21 parts of lauryl alcohol ester.

[0020] 1) Mix 35 parts of barium hydroxide, 20 parts of zinc oxide, 15 parts of aluminum naphthenate soap, 7 parts of barium chromate, 22 parts of ceramic micropowder, 9 parts of silicon carbide, 50 parts of phenolic epoxy resin, 3 parts of aluminum phosphate, 7 parts of polyvinyl butyral and 6 parts of...

Embodiment 2

[0026] An anti-corrosion coating for doors is made of the following materials in parts by weight: 37.5 parts of barium hydroxide, 22.5 parts of zinc oxide, 17.5 parts of aluminum naphthenate soap, 8 parts of barium chromate, 23 parts of ceramic micropowder, 12 parts of silicon carbide, 52.5 parts of phenolic epoxy resin, 4 parts of aluminum phosphate, 8.5 parts of polyvinyl butyral, 7.5 parts of butadiene resin film former, 6 parts of acrylic resin, 3.5 parts of mica, phytic acid ester 5.5 parts, 13 parts of chlorinated paraffin, 7.5 parts of toluenesulfonic acid, 7 parts of lithopone, 12.5 parts of biuret, 24 parts of polysiloxane, 9 parts of cooked tung oil and 18.5 parts of lauryl alcohol ester.

[0027] 1) 37.5 parts of barium hydroxide, 22.5 parts of zinc oxide, 17.5 parts of aluminum naphthenate soap, 8 parts of barium chromate, 23 parts of ceramic micropowder, 12 parts of silicon carbide, 52.5 parts of novolac epoxy resin, 4 parts of aluminum phosphate, 8.5 parts of pol...

Embodiment 3

[0033]An anti-corrosion coating for doors is made of the following materials in parts by weight: 40 parts of barium hydroxide, 25 parts of zinc oxide, 20 parts of aluminum naphthenate soap, 9 parts of barium chromate, 24 parts of ceramic micropowder, 15 parts of silicon carbide, 55 parts of phenolic epoxy resin, 5 parts of aluminum phosphate, 10 parts of polyvinyl butyral, 9 parts of butadiene resin film former, 8 parts of acrylic resin, 5 parts of mica, phytic acid ester 8 parts, 14 parts of chlorinated paraffin, 9 parts of toluenesulfonic acid, 8 parts of lithopone, 14 parts of biuret, 26 parts of polysiloxane, 10 parts of cooked tung oil and 21 parts of lauryl alcohol ester.

[0034] 1) Mix 40 parts of barium hydroxide, 25 parts of zinc oxide, 20 parts of aluminum naphthenate soap, 9 parts of barium chromate, 24 parts of ceramic micropowder, 15 parts of silicon carbide, 55 parts of phenolic epoxy resin, 5 parts of aluminum phosphate, 10 parts of polyvinyl butyral and 9 part...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses an anticorrosive paint for a door. The anticorrosive paint is prepared from the following materials in parts by weight: 35-40 parts of barium hydroxide, 20-25 parts of zinc oxide, 15-20 parts of aluminium naphthenate, 7-9 parts of barium chromate, 22-24 parts of ceramic micro-powder, 9-15 parts of silicon carbide, 50-55 parts of novolac epoxy resin, 3-5 parts of aluminium phosphate, 7-10 parts of polyvinyl butyral, 6-9 parts of butadiene resin film former, 4-8 parts of acrylic resin, 2-5 parts of mica, 3-8 parts of inositol hexaphosphate, 12-14 parts of chlorinated paraffin, 8-9 parts of toluenesulfonic acid, 6-8 parts of lithopone, 11-14 parts of biuret, 22-26 parts of polysiloxane, 8-10 parts of boiled wood oil, and 16-21 parts of 2,2,4-trimethyl-1,3-pentanediol monoisobutyrate. The anticorrosive paint for the door has good anticorrosion performance, is resistant to high temperature, has an insulating effect, and can keep long life of the coating.

Description

technical field [0001] The invention relates to a door anticorrosion coating and a preparation method thereof. Background technique [0002] Anti-corrosion coatings, generally divided into conventional anti-corrosion coatings and heavy-duty anti-corrosion coatings, are an indispensable coating in paint coatings. Conventional anti-corrosion coatings play an anti-corrosion effect on metals under normal conditions and protect the service life of non-ferrous metals; A type of anti-corrosion coating that achieves a longer protection period than conventional anti-corrosion coatings. Main categories: Inorganic zinc silicate shop primer, inorganic zinc silicate shop primer (high zinc), water-based inorganic zinc-rich primer, water-based inorganic zinc-rich primer (high zinc), vinyl phosphating primer, various colors of silicone Heat-resistant paint (300℃), silver silicone heat-resistant paint (400℃), white alkyd hull paint, black alkyd hull paint, green alkyd hull paint, blue gray...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D163/04C09D129/04C09D133/00C09D183/04C09D147/00C09D7/12C09D5/03
CPCC09D163/04C08K2201/014C08L2201/08C08L2205/02C08L2205/035C09D5/08C09D5/18C09D7/61C09D7/63C09D7/65C08L29/14C08L33/00C08L47/00C08L91/06C08L83/04C08L91/00C08K13/02C08K2003/2296C08K2003/2206C08K5/098C08K3/24C08K3/34
Inventor 洪长林
Owner ANHUI KATA DOOR & WINDOW
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products