Self-leveling dry-mixed mortar and preparation method thereof
A dry-mixed mortar and self-leveling technology, applied in the field of building materials, can solve the problems of low early strength, long setting time, weak industrial load-bearing capacity, etc., and achieve improved strength and wear resistance, smooth surface, and simple preparation process. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0045] In a second aspect, the present invention provides a method for preparing self-leveling dry-mixed mortar, comprising the following steps: weighing raw materials according to the above-mentioned self-leveling dry-mixed mortar, and then mixing ordinary Portland cement, steel slag, and phosphogypsum Mix and stir with sepiolite powder evenly, then add high-efficiency water reducer, defoamer, carboxypropyl methyl cellulose ether, fly ash, basalt fiber and redispersible latex powder, mix and stir evenly to obtain the self-leveling dry Mixed mortar.
[0046] The self-leveling dry-mixed mortar has a simple preparation process and low cost. The self-leveling dry-mixed mortar prepared by this method has the advantages of high strength, smooth and flat surface after condensation, good wear resistance, low cost and good environmental protection.
Embodiment 1
[0049] A self-leveling dry-mixed mortar, comprising the following raw materials in parts by weight: 20 parts of ordinary Portland cement, 30 parts of steel slag, 1 part of phosphogypsum, 1 part of sepiolite powder, 0.1 part of high-efficiency water reducer, and 0.1 part of defoamer , 0.1 part of carboxypropyl methylcellulose ether, 1 part of fly ash, 0.1 part of basalt fiber and 0.1 part of vinyl acetate-ethylene copolymer rubber powder;
[0050] Among them, the strength grade of ordinary Portland cement is 42.5, the particle size of steel slag is 20 μm, the particle size of fly ash is 10 μm, the diameter of basalt fiber is 3 μm, the length is 3 mm, and the defoamer is THIX-568 cement mortar defoamer (Yantai Hengxin Chemical Technology Co., Ltd.).
Embodiment 2
[0052] A self-leveling dry-mixed mortar, comprising the following raw materials in parts by weight: 20 parts of ordinary Portland cement, 30 parts of steel slag, 1 part of phosphogypsum, 1 part of sepiolite powder, 0.1 part of high-efficiency water reducer, and 0.1 part of defoamer , 0.1 part of carboxypropyl methylcellulose ether, 1 part of fly ash, 0.1 part of basalt fiber and 0.1 part of ethyl acetate-ethylene-higher fatty acid ethylene ester ternary copolymer rubber powder;
[0053] Among them, the strength grade of ordinary Portland cement is 42.5, the particle size of steel slag is 18 μm, the particle size of fly ash is 10 μm, the diameter of basalt fiber is 8 μm, the length is 5 mm, and the defoamer is THIX-568 cement mortar defoamer (Yantai Hengxin Chemical Technology Co., Ltd.).
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| particle size | aaaaa | aaaaa |
| diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.