Embodiment 1
[0031] An amorphous dressing for scald wounds containing snake oil, comprising the following raw materials in parts by weight:
[0032] Aloe extracts 100 parts of mucus (water content 26wt%), 4 parts of polyethylene glycol, 4 parts of snake oil, 3 parts of Cortex Phellodendri, 2 parts of camphor, 2 parts of sodium carboxymethyl cellulose, antibacterial agent (by mass ratio being 2 : 1.5:2 magnesium nitrate, iron nitrate and copper nitrate) 1 part, 50 parts alcohol, 3 parts sodium carbonate, 5 parts citric acid.
[0033] The preparation method of the above-mentioned amorphous dressing for scald wound containing snake oil, the steps are as follows:
[0034] (a) Add polyethylene glycol, snake oil, cork cork, camphor, sodium carboxymethylcellulose, and antibacterial agent to the mucus extracted from aloe vera in sequence, and stir evenly to obtain a viscous mixed mucus.
[0035] (b) Under the conditions of low-speed stirring (150r / min) and 3°C, add sodium carbonate and citric aci...
Embodiment 2
[0039] An amorphous dressing for scald wounds containing snake oil, comprising the following raw materials in parts by weight:
[0040] Aloe extracts 100 parts of mucus (water content 26wt%), 4 parts of polyethylene glycol, 4 parts of snake oil, 3 parts of Cortex Phellodendri, 2 parts of camphor, 2 parts of sodium carboxymethyl cellulose, antibacterial agent (by mass ratio being 2 : 1.5:2 magnesium nitrate, iron nitrate and copper nitrate) 1 part, 50 parts alcohol, 3 parts sodium carbonate, 5 parts citric acid.
[0041] Among them, the snake oil is subjected to load treatment before adding: take the snake oil and heat it to 80°C to make it liquid; then add 0.5 times its mass of fumed hydrophobic silica powder to the snake oil, stir evenly, and get the load Processed snake oil.
[0042] The preparation method of the gas-phase hydrophobic silica powder is as follows: dilute tetraethyl orthosilicate 45 times with 80wt% alcohol solution, after mixing evenly, add acetic acid solut...
Embodiment 3
[0049] An amorphous dressing for scald wounds containing snake oil, comprising the following raw materials in parts by weight:
[0050] Aloe extracts 90 parts of mucus (water content 20wt%), 7 parts of polyethylene glycol, 3 parts of snake oil, 4 parts of Cortex Phellodendri, 1 part of camphor, 3 parts of sodium carboxymethyl cellulose, antibacterial agent (by mass ratio of 2 : 1:2 magnesium nitrate, iron nitrate and copper nitrate) 0.5 parts, alcohol 40 parts, sodium carbonate 2 parts, citric acid 3 parts.
[0051] Among them, the snake oil is subjected to load treatment before adding: take the snake oil and heat it to 70°C to make it liquid; then add 0.4 times its mass of gas-phase hydrophobic silica powder to the snake oil, stir evenly, and get the load Processed snake oil.
[0052] The preparation method of the gas-phase hydrophobic silica powder is as follows: dilute tetraethyl orthosilicate 40 times with 80wt% alcohol solution, after mixing evenly, add acetic acid solut...