Polymer composite material with high gas-liquid barrier performance and preparation method thereof
A technology of composite materials and polymers, applied in coatings and other directions, can solve problems such as insufficient resistance to mechanical damage, and achieve good mechanical stability, no deterioration of structural properties, and high water resistance and waterproof performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0064] Polymer composite
[0065] The polymer composite material includes a polymer substrate layer composed of polyethylene terephthalate. Polyacrylic acid with a molecular weight of 5000~50,000g / mol is chemically grafted on the substrate layer by superheated hydrogen treatment as a modified layer, and a composite coating of graphene oxide and silicone rubber polymer is combined on the outermost surface of the composite material as a barrier function Floor. Among them, the graphene oxide sheet has a diameter of 5-15 microns and the number of layers is 2-5.
Embodiment 2
[0067] Polymer composite
[0068] The polymer composite material includes a polymer substrate layer composed of polychlorinated p-xylene. Polyethylene glycol with a molecular weight of 10,000 to 100,000 g / mol chemically grafted on the substrate layer by superheated hydrogen treatment is used as a modified layer, and graphene oxide and silicone rubber polymer composite coating is combined on the outermost surface of the composite material as a The barrier function layer. Among them, the graphene oxide sheet has a diameter of 1-40 microns and the number of layers is 1-10.
Embodiment 3
[0070] Preparation of polymer composites
[0071] Step (1) Pretreatment of the polymer substrate layer. The polyethylene film was soaked in ethanol for 60 minutes, and then dried at 90°C for 10 minutes; then soaked in deionized water for 10 minutes, and then dried at 90°C for 10 minutes; then treated with low-temperature plasma for 10 seconds.
[0072] Step (2) coating and grafting treatment of the modified layer. Polyacrylic acid (the second polymer) with a molecular weight of 2000 g / mol was dissolved in water to prepare a modified layer raw material solution with a mass concentration of 8.5%, and ultrasonically dispersed for 10 minutes. Then, the dispersion was coated on the polyethylene substrate layer pretreated in step (1) by dip coating for 3600s, and then dried at 50°C for 10 minutes, and then superheated at a voltage of 100V and a vacuum of 0.05Pa. After being processed for 100s in the hydrogen plant, take it out for use.
[0073] Step (3) Preparation of barrier functiona...
PUM
Property | Measurement | Unit |
---|---|---|
molecular weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com