Method for restoring steep slopes of mining area by mechanical spraying of lime neutralizing sludge slag
A lime and mechanical technology, applied in the field of ecological restoration in mining areas, can solve the problems of clogging, lime neutralization and sludge powder adhesion, etc., and achieve the effect of reducing viscosity, saving energy consumption, and overcoming adhesion of pipes or blockages.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] Lime-neutralized sludge is iron-containing acidic wastewater formed in the process of wet copper smelting in copper sulfide mines. It is treated by lime neutralization method. The neutralized slurry is filtered by plate and frame. The moisture content of lime-neutralized sludge is 34.35%. , the mass ratio of ultra-fine particles with a particle size of less than 0.045mm exceeds 97.11%, and after natural drying and mechanical crushing, the moisture content is reduced to 15.51%.
[0032] Flotation tailings slag refers to the flotation tailings slag with low sulfur content produced after the copper sulfide ore is flotation-recovered first, and then the copper-separated tailings are subjected to the flotation and sulfur-selection process. The quartz content is 78.12%, and the clay minerals The content is 1.72%, the water content is 12.55%, the sulfur content is 0.25%, the particle size range is 0.01-16mm, and the mass ratio of particles with a particle size of 0.5-16mm is 68...
Embodiment 2
[0036] Lime-neutralized sludge is the acid-containing and iron-containing acidic wastewater formed in the process of wet copper smelting in copper sulfide mines. It is treated by lime neutralization method. The neutralized slurry is filtered through plate and frame. 39.49%, the mass ratio of ultra-fine particles with a particle size of less than 0.045mm exceeds 99.42%, and after natural drying and mechanical crushing, the moisture content is reduced to 23.72%.
[0037]Flotation tailings slag refers to the flotation tailings slag with low sulfur content produced after the copper sulfide ore is flotation-recovered first, and then the copper-separated tailings are subjected to the flotation sulfur-selection process. The quartz content is 87.17%, and the clay minerals The content is 2.29%, the water content is 12.12%, the particle size is 0.01-20mm, the sulfur content is 0.14%, and the mass ratio of particles with a particle size of 0.5-20mm is 73.34%.
[0038] First, neutralize t...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com