Preparation method of calcium chloride solution for fluorite mine beneficiation wastewater treatment
A technology for calcium chloride solution and beneficiation wastewater, applied in mining wastewater treatment, chemical instruments and methods, water/sludge/sewage treatment, etc., can solve problems such as high freight, low lime solubility, cumbersome process, etc., and reduce production The effect of cost, simplification of conventional preparation process and simplification of treatment process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A method for preparing calcium chloride solution for fluorite mineral processing wastewater treatment, comprising the following steps:
[0023] (1) Take lime and hydrochloric acid as raw materials, add them to the reactor for stirring reaction, and filter the reactants when the pH value of the reaction system is 4.5;
[0024] (2) In the filtrate obtained in step (1), first add ammonia triacetamide of 0.02% of the total mass of calcium chloride in the filtrate, and then add calcium chloride solid to prepare a calcium chloride solution with a mass concentration of 53.5%;
[0025] (3) Add polyaluminum chloride and citric acid to the solution obtained in step (2), the amount of polyaluminum chloride added is 2% of the total mass of calcium chloride in the solution, and the amount of malic acid added is 2% of the total mass of calcium chloride in the solution 0.03% of the total mass, stirred evenly, and aged for 2 hours to obtain the product.
Embodiment 2
[0027] A method for preparing calcium chloride solution for fluorite mineral processing wastewater treatment, comprising the following steps:
[0028] (1) Take lime and hydrochloric acid as raw materials, add them to the reactor for stirring reaction, and filter the reactants when the pH value of the reaction system is 5;
[0029] (2) In the filtrate obtained in step (1), first add ammonia triacetamide of 0.03% of the total mass of calcium chloride in the filtrate, and then add calcium chloride solid to prepare a calcium chloride solution with a mass concentration of 55.2%;
[0030] (3) Add polyaluminum chloride and citric acid to the solution obtained in step (2), the addition of polyaluminium chloride is 2.5% of the total mass of calcium chloride in the solution, and the addition of acetic acid is the total mass of calcium chloride in the solution 0.05% of the mass, stirred evenly, and aged for 2 hours to obtain the product.
Embodiment 3
[0032] A method for preparing calcium chloride solution for fluorite mineral processing wastewater treatment, comprising the following steps:
[0033] (1) Take lime and hydrochloric acid as raw materials, add them to the reactor for stirring reaction, and filter the reactants when the pH value of the reaction system is 4.5;
[0034] (2) In the filtrate obtained in step (1), first add ammonia triacetamide of 0.05% of the total mass of calcium chloride in the filtrate, and then add calcium chloride solid to prepare a calcium chloride solution with a mass concentration of 57.0%;
[0035] (3) Add polyaluminum chloride and citric acid to the solution obtained in step (2), the amount of polyaluminum chloride added is 3.0% of the total mass of calcium chloride in the solution, and the amount of citric acid added is 3.0% of the total mass of calcium chloride in the solution 0.07% of the total mass, stirred evenly, and aged for 2 hours to obtain the product.
[0036] Calcium chloride ...