POK/PET/PBT (polyketone/polyethylene terephthalate/polybutylene terephthalate) ternary alloy material and preparation process thereof
A ternary alloy and compatibilizer technology, applied in the field of POK/PET/PBT ternary alloy material and its preparation process, can solve the problem of poor antistatic performance and flame retardancy, and adjust POK/PET/PBT ternary alloy material Toughness and hardness, limit the scope of use and other issues, to achieve good dimensional stability, good processing performance, increase the effect of practicality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The invention provides a technical solution: a POK / PET / PBT ternary alloy material, the components of which are proportioned by mass percentage: polyethylene terephthalate 25%, polybutylene terephthalate 30% ester, 20% polyketone, 5% antistatic agent, 10% halogen-free flame retardant, 0.5% compatibilizer, 0.5% lubricant, 5% antioxidant, 1% toughening agent and 3% reinforcing agent.
[0024] In the present invention: the antistatic agent is an antistatic agent formed by compounding alkylbenzene sulfonate and siloxane, and the mass ratio of alkylbenzene sulfonate and siloxane in the antistatic agent is 7:2.
[0025] In the present invention: the toughening agent is a mixture of methyl methacrylate-butadiene-styrene terpolymer and acrylonitrile-butadiene-styrene copolymer.
[0026] In the present invention: the compatibilizer is a mixture of a cyclic anhydride type compatibilizer and an isocyanate type compatibilizer.
[0027] In the present invention: the halogen-free fla...
Embodiment 2
[0034] Embodiment 2: This implementation differs from Embodiment 1 in that:
[0035] The invention provides a technical solution: a POK / PET / PBT ternary alloy material, the components of which are proportioned by mass percentage: polyethylene terephthalate 30%, polybutylene terephthalate 30% ester, 20% polyketone, 4% antistatic agent, 9% halogen-free flame retardant, 0.2% compatibilizer, 0.8% lubricant, 3% antioxidant, 1% toughening agent and 2% reinforcing agent.
[0036] In the present invention: the antistatic agent is an antistatic agent formed by compounding alkylbenzene sulfonate and siloxane, and the mass ratio of alkylbenzene sulfonate and siloxane in the antistatic agent is 8:3.
[0037] In the present invention: the toughening agent is a mixture of styrene-butadiene thermoplastic elastomer and polyimide.
[0038] In the present invention: the compatibilizer is a mixture of epoxy resin type compatibilizer, oxazoline type compatibilizer and isocyanate type compatibiliz...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com