A water supply pipeline and anti-corrosion technology, applied in the field of pipelines, can solve the problems of poor corrosion resistance, reduced pipeline strength, low compressive strength, etc., and achieve the effects of reducing production costs, improving overall performance, and improving overall strength.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Such as figure 1 , figure 2 They are respectively a structural schematic diagram and a cross-sectional structural schematic diagram of the present invention, including a metal pipe 1 and a coating 2 located on the inner wall of the metal pipe, the coating includes an epoxy resin coating 21 and a water-based polyurethane coating 22, and the ring The epoxy coating sits between the metal pipe and the water-based polyurethane coating.
[0024] The preparation method of modified basalt scales comprises the following steps:
[0025]Add 3g of acrylic acid and 1.5g of 1,4-butenediol into 150mL of deionized water and stir to dissolve, add 0.05g of surfactant sodium lauryl sulfate and 2mL of 10% sodium hydroxide aqueous solution, stir and mix to obtain Mixed liquid, set aside; add 3g of basalt scales to 200mL of piperazine aqueous solution with a mass concentration of 5%, add 0.08g of surfactant sodium lauryl sulfate, ultrasonically vibrate for 30min with 200W power, filter an...
Embodiment 2
[0033] The anti-corrosion water supply pipeline includes a metal pipeline 1 and a coating 2 on the inner wall of the metal pipeline. The coating includes an epoxy resin coating 21 and a water-based polyurethane coating 22. The epoxy resin coating is located between the metal pipeline and the water-based between coats of polyurethane.
[0034] The preparation method of modified basalt scales comprises the following steps:
[0035] Add 3g of acrylic acid and 0.6g of 1,4-butenediol into 150mL of deionized water and stir to dissolve, add 0.05g of surfactant sodium lauryl sulfate and 2mL of 10% sodium hydroxide aqueous solution, stir and mix to obtain Mixed solution, set aside; add 3g of basalt scales to 200mL of piperazine aqueous solution with a mass concentration of 1%, add 0.08g of surfactant sodium lauryl sulfate, ultrasonically vibrate for 20min with 200W power, filter and separate the basalt scales; put the basalt The scales were added to 250 mL of n-hexane solution with a ...