A sewage treatment and river channel technology, applied in water/sewage treatment, biological water/sewage treatment, light water/sewage treatment, etc., can solve the problems of multiple organic pollutants and incomplete effects, and achieve high removal rate and good removal Odor and decolorization effect, strong adsorption effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] Embodiment 1: the preparation of vermiculite / diatomite / activated carbon composite adsorbent
[0026] Vermiculite / diatomite / activated carbon composite adsorbent is prepared by the following method:
[0027] Weigh 28 parts of vermiculite powder and 18 parts of diatomaceous earth, mix them uniformly, and place them at 500°C for 90 minutes to calcinate to obtain a calcined mixed powder; add 15% of the total mass of starch and an appropriate amount of water to the calcined mixed powder, and mix well , to make granular materials with a particle size of 2-3mm, and then place them in an oven at 80-85°C to dry them, then calcinate them at 780°C for 2.5 hours under the protection of inert gas, and cool them with the furnace under the protection of inert gas to room temperature, and then pulverized to below 30 mesh to obtain the vermiculite / diatomaceous earth / activated carbon composite adsorbent.
Embodiment 2
[0028] Embodiment 2: the preparation of vermiculite / diatomite / activated carbon composite adsorbent
[0029] Vermiculite / diatomite / activated carbon composite adsorbent is prepared by the following method:
[0030] Weigh 20 parts of vermiculite powder and 15 parts of diatomaceous earth, mix them evenly, and place them at 450°C for 60-90 minutes to calcinate to obtain a calcined mixed powder; add 20% of the total mass of starch and an appropriate amount of water to the calcined mixed powder, Mix evenly to make granular materials with a particle size of 2-3mm, then dry them in an oven at 80-85°C, then calcinate at 720°C for 2 hours under the protection of an inert gas, and carry them into the furnace under the protection of an inert gas. Cool to room temperature, and then pulverize to below 30 mesh to obtain vermiculite / diatomaceous earth / activated carbon composite adsorbent.
Embodiment 3
[0031] Embodiment 3: Preparation of photocatalyst nickel-doped nano-titanium dioxide
[0032] The photocatalyst nickel-doped nano-titanium dioxide is prepared by the following method:
[0033] Mix butyl titanate with nickel nitrate hexahydrate, absolute ethanol, and water evenly, and then slowly add glacial acetic acid dropwise while vigorously stirring; continue stirring for 1 hour after the glacial acetic acid is dripped, let the resultant stand for 5 hours, and place in 60 Dry at -70°C to constant weight, grind and place in a muffle furnace, calcinate at 720°C for 3.5 hours, cool to room temperature, grind and sieve to obtain nickel-doped nano-titanium dioxide.
[0034] Among them, the mass ratio of butyl titanate, nickel nitrate hexahydrate, absolute ethanol, water, and glacial acetic acid is 1:0.1:8:0.8:0.5.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com