A film base material and one-way guide technology, which is applied in rayon manufacturing, single-component polyester rayon, fiber treatment, etc., can solve the problem of short duration of one-way water guide effect, unsuitable for use of mask materials, unfavorable environment and Human health and other issues, to achieve the effect of excellent water absorption and water retention, comfortable and soft touch, and excellent overall performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example 1
[0036] Add terephthalic acid, butylene glycol, and castor oil modified polyols into the reaction kettle, the molar ratio of terephthalic acid, butylene glycol, and castor oil modified polyols is 120:100:10. , the relative pressure is prepolymerization 1h under-0.05MPa; Then add the polycondensation catalyst Sb of monomer (the sum of terephthalic acid, butanediol, castor oil modified polyol) 1wt% 2 o 3 , at 270°C, 0.01MPa polycondensation for 5h, the acid value of the detection system is lower than 10mg KOH / g, stop the reaction, filter to remove impurities, pass through the casting belt, and use a dicing machine to slice the polyester, and measure the viscosity average of the obtained polyester The molecular weight is 23400 g / mol.
[0037] The resulting 100 parts of polyester chips and 7 parts of PEG600, 0.5 parts of nano-silver, 1.1 parts of pentaerythritol stearate, 0.8 parts of antioxidant 2246 are added to a twin-screw extruder for extrusion granulation, twin-screw extrude...
preparation example 2
[0040] Other conditions and steps are the same as those in Preparation Example 1, except that the molar ratio of castor oil-modified polyol to terephthalic acid, butylene glycol, and castor oil-modified polyol is 120:100:5.
preparation example 3
[0042] After the polyvinyl alcohol fiber is soaked with chitosan acetic acid solution for 4 hours, wherein the concentration of chitosan is 3wt%, and the concentration of acetic acid is 6wt%, it is taken out and dried to obtain the chitosan modified polyvinyl alcohol fiber.
PUM
Property | Measurement | Unit |
---|---|---|
hydroxyl value | aaaaa | aaaaa |
acid value | aaaaa | aaaaa |
hydroxyl value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com