Silver ion long-acting sterilization wall coating and preparation method thereof
A silver ion, long-acting technology, applied in the field of coatings, can solve the problems of human liver injury, inhalation, etc., achieve the effect of inhibiting Aspergillus niger, improving stability, and increasing use value
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0056] The second aspect of the present invention provides a method for preparing a silver ion long-acting bactericidal wall coating, comprising the following steps:
[0057] 1) Add active group-containing monomers into water, then add surfactant and silver ion water and stir and mix;
[0058] 2) Add coupling agent, filler, film-forming agent and defoamer to step 1), stir, and react for 1-3 hours to obtain.
Embodiment 1
[0062] A silver ion long-acting bactericidal wall paint, the raw materials for preparation include: 1% electrolytic silver water, 50% water-based polyurethane monomer, 0.5% surfactant, 1% filler, 0.1% coupling agent, 2 , 2,4-trimethyl-1,3-pentanediol monoisobutyrate 0.1%, defoamer 0.1%, water to add the balance to 100%.
[0063] The mass concentration of the electrolytic silver water is 25ppm.
[0064] The surfactant is selected from coconut oil fatty acid diethylamide and C12-14 alkyl glycoside, and its weight ratio is 1:0.1.
[0065] The filler is selected from calcium carbonate with a particle size of 4000 mesh and 6250 mesh, and its weight ratio is 1:2.5.
[0066] The coupling agent is selected from isopropyl tris (dioctyl pyrophosphate acyloxy) phthalate and isopropyl tris (dioctyl phosphate acyloxy) phthalate, and its weight ratio is 1:0.1 .
[0067] The defoamer is selected from silicone defoamers, model GS-5820, purchased from Shanghai Zicheng International Trade Co...
Embodiment 2
[0073] A silver ion long-acting bactericidal wall paint, the raw materials for preparation include: electrolytic silver water 3%, water-based polyurethane monomer 70%, surfactant 2%, filler 2%, coupling agent 3%, 2% by weight. , 2,4-trimethyl-1,3-pentanediol monoisobutyrate 1%, defoamer 1%, water to add the balance to 100%.
[0074] The mass concentration of the electrolytic silver water is 25ppm.
[0075] The surfactant is selected from coconut oil fatty acid diethylamide and C12-14 alkyl glucoside, and its weight ratio is 1:0.5.
[0076] The filler is selected from calcium carbonate with a particle size of 4000 mesh and 6250 mesh, and its weight ratio is 1:4.
[0077] The coupling agent is selected from isopropyl tris (dioctyl pyrophosphate acyloxy) phthalate and isopropyl tris (dioctyl phosphate acyloxy) phthalate, and its weight ratio is 1:0.5 .
[0078] The defoamer is selected from silicone defoamers, model GS-5820, purchased from Shanghai Zicheng International Trade ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com