Method for preparing absorbent fibrin hemostatic plaster
A technology for absorbing fiber and fibrinogen, applied in the field of medical devices, can solve the problems of organ shedding, failure to meet clinical needs, time-consuming, etc., achieve good biocompatibility, improve hemostatic effect, and have no toxic and side effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] (1) Take 1 milligram of riboflavin, 950 milligrams of fibrinogen and 475 active units of thrombin freeze-dried powder, add them into a mortar and grind thoroughly, wherein the fibrinogen and thrombin are from pig blood;
[0031] (2) Add 100 milliliters of dehydrated ethanol to the above-mentioned uniformly mixed dry powder and stir to form a uniform suspension, and vibrate to evenly distribute the suspended particles;
[0032] (3) Pour the evenly distributed suspension into a 10×20 square centimeter flat bottom pan, make one side of the collagen sponge contact the suspension, and the particles in the suspension adhere to the collagen sponge;
[0033] (4) Vacuum-dry the collagen sponge adhered with mixed dry powder particles, cut according to predetermined specifications, and sterilize by cobalt source irradiation after vacuum-tight packaging.
Embodiment 2
[0035] (1) Take 1 mg of riboflavin, 1000 mg of fibrinogen and 250 active units of freeze-dried thrombin powder, add them into a mortar and grind thoroughly, wherein the fibrinogen and thrombin are taken from human blood;
[0036] (2) Add 100 milliliters of dehydrated ethanol to the above-mentioned uniformly mixed dry powder and stir to form a uniform suspension, and vibrate to evenly distribute the suspended particles;
[0037] (3) Pour the evenly distributed suspension into a 10×20 square centimeter flat bottom pan, make one side of the collagen sponge contact the suspension, and the particles in the suspension adhere to the collagen sponge;
[0038] (4) Vacuum-dry the collagen sponge adhered with mixed dry powder particles, cut according to predetermined specifications, and sterilize by cobalt source irradiation after vacuum-tight packaging.
Embodiment 3
[0040] (1) Take 1 milligram of riboflavin, 1100 milligrams of fibrinogen and 300 active units of thrombin freeze-dried powder, add them into a mortar and grind them thoroughly, wherein the fibrinogen and thrombin are taken from bovine blood;
[0041] (2) Add 100 milliliters of dehydrated ethanol to the above-mentioned uniformly mixed dry powder and stir to form a uniform suspension, and vibrate to evenly distribute the suspended particles;
[0042] (3) Pour the uniformly distributed suspension into a 10 × 20 square centimeter flat pan, make one side of the collagen sponge contact the suspension, and the particles in the suspension adhere to the collagen sponge;
[0043] (4) Vacuum-dry the collagen sponge adhered with mixed dry powder particles, cut according to predetermined specifications, and sterilize by cobalt source irradiation after vacuum-tight packaging.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com