A degreaser and solvent technology, applied in the field of degreaser, can solve the problems of metal paint and skin corrosion, environmental pollution, human body infringement, etc., achieve significant economic and social benefits, scientific and reasonable composition, and good cleaning effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0025] Example 1
[0026] The present invention is made by mixing and emulsification of the raw materials of the following weight proportions:
[0027] 400Kg of small molecular water, 100Kg of bis(dilauryl phosphite) tetraoctyltitanium, and 100Kg of fatty acid ethylene oxide adduct, which were statically treated with the active water device with product standard number of YZB / Ganhong 0112-2003 for 4 hours , 200 # Solvent oil 200Kg, composite surfactant 200Kg;
[0028] Wherein the compounding surfactant weight ratio is:
[0029] Japan-made nonylphenol polyoxyethylene ether HA-100 57.3%, Japan-made nonylphenol polyoxyethylene ether sulfonic acid ES-204 2.7%.
[0030] The two can be mixed evenly.
[0031] Preparation:
[0032] After the ingredients are mixed, the temperature is raised to 75±2° C., and the mixture is transported to an emulsifying machine for emulsifying treatment to obtain the degreasing agent of the present invention.
Example Embodiment
[0033] Example 2
[0034] The present invention is made by mixing and emulsification of the raw materials of the following weight proportions:
[0035] Small molecule water 350Kg, bis(dilauryl phosphite) tetraoctyl titanium oxide 90Kg, fatty acid ethylene oxide adduct 106Kg, 200 # Solvent oil 180Kg, composite surfactant 190Kg;
[0036] Wherein the compounding surfactant weight ratio is:
[0037] Nonylphenol polyoxyethylene ether HA-100 56%, nonylphenol polyoxyethylene ether sulfonic acid ES-20 45%.
[0038] Preparation:
[0039] The ingredients are added into the reaction kettle, and after mixing, the temperature is raised to 75±1° C., and the mixture is transported to an emulsifying machine for emulsifying treatment to obtain the degreasing agent of the present invention.
Example Embodiment
[0040] Example 3
[0041] The present invention is made by mixing and emulsification of the raw materials of the following weight proportions:
[0042] Small molecule water 360Kg, bis(dilauryl phosphite) tetraoctyl titanium 85Kg, fatty acid ethylene oxide adduct 100Kg, 200 # Solvent oil 200Kg, composite surfactant 190Kg;
[0043] Wherein the compounding surfactant weight ratio is:
[0044] Nonylphenol polyoxyethylene ether HA-100 58%, nonylphenol polyoxyethylene ether sulfonic acid ES-20 42%.
[0045] Preparation:
[0046] After the ingredients are mixed, the temperature is raised to 74±2° C., and the mixture is transported to an emulsifying machine for emulsifying treatment to obtain the degreasing agent of the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap