Process for hydrothermal synthesizing bismuth citrate

A technology of bismuth citrate and hydrothermal synthesis, applied in the preparation of carboxylate, organic chemistry and other directions, can solve the problems of low atomic economy, increased product toxicity, unfriendly environment, etc., and achieve green production process, increase One-time utilization, environment-friendly effect

Inactive Publication Date: 2006-06-28
EAST CHINA NORMAL UNIV
View PDF0 Cites 9 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Therefore, it is easy to mix nitrate ions in the product, which increases the toxicity of the product
At the same time, the reaction requires twice the excess of citric acid, and the atom e

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] Step 1: Grind 1 mmol of bismuth oxide and 2.1 mmol of citric acid in a mortar until they are evenly mixed, put them into an autoclave, and add 4 mmol of water. The autoclave was sealed well, placed in a constant temperature drying oven, and reacted at a constant temperature for 6 hours at a set temperature of 140°C.

[0018] Step 2: Take out the autoclave, open it after it cools down naturally, take out the suspension in the autoclave and filter it with suction, wash the filter cake with distilled water until the pH of the filtrate is 5-7, and there is no citric acid.

[0019] The third step is to put the obtained solid into a vacuum drying oven at 60° C. for vacuum drying to obtain pure bismuth citrate. Calculated by adding bismuth oxide, the yield of bismuth citrate can reach 99%.

Embodiment 2

[0021] Step 1: Grind 1 mmol of bismuth oxide and 2.1 mmol of citric acid in a mortar until they are evenly mixed, put them into an autoclave, and add 4 mmol of water. The autoclave was sealed well, placed in a constant temperature drying oven, and reacted at a constant temperature for 9 hours at a set temperature of 130°C.

[0022] Step 2: Take out the autoclave, open it after it cools down naturally, take out the suspension in the autoclave and filter it with suction, wash the filter cake with distilled water until the pH of the filtrate is 5-7, and there is no citric acid.

[0023] The third step is to put the obtained solid into a vacuum drying oven at 60° C. for vacuum drying to obtain pure bismuth citrate. Calculated by adding bismuth oxide, the yield of bismuth citrate can reach 99%.

Embodiment 3

[0025] Step 1: Grind 2mmol of bismuth oxide and 4.2mmol of citric acid in a mortar until they are evenly mixed, put them into an autoclave, and add 8mmol of water. The autoclave was sealed well, placed in a constant temperature drying oven, and reacted at a constant temperature for 12 hours at a set temperature of 120°C.

[0026] Step 2: Take out the autoclave, open it after it cools down naturally, take out the suspension in the autoclave and filter it with suction, wash the filter cake with distilled water until the pH of the filtrate is 5-7, and there is no citric acid.

[0027] The third step is to put the obtained solid into a vacuum drying oven at 60° C. for vacuum drying to obtain pure bismuth citrate. Calculated by adding bismuth oxide, the yield of bismuth citrate can reach 99%.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a method to compounding citron acid bismuth by hydrothermal. It adopts bismuth oxide and citron acid by hydrothermal compounding and filtering and drying to gain citron acid bismuth. The result of the invention has high purity, fully reaction high atom economical efficiency, short reaction time. It has no harmful to environment.

Description

technical field [0001] The invention relates to the technical field of inorganic coordination chemistry synthesis, in particular to a method for hydrothermally synthesizing bismuth citrate (also known as bismuth citrate, Bismuth Citrate). Background technique [0002] Citric acid is also called citric acid. Bismuth citrate is a pharmaceutical intermediate for the synthesis of various drugs in the pharmaceutical industry. Bismuth citrate is an essential raw material in the preparation of many drugs for the treatment of digestive tract diseases. For example: Colloidal Bismuth Subcitrate (CBS, De-Nol E ; Livzon Dele, China), ranitidine bismuth citrate (Ranitidine Bismuth Citrate, RBS, Pylorid). Bismuth citrate supermolecules can act on the surface of gastric ulcer membrane and have certain biological activity. At the same time, bismuth citrate supermolecules can bind to the position of zinc and iron in the protein to inhibit the growth of bacteria. The traditional method of...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C07C51/41C07C59/265
Inventor 单永奎王一蕾赖克强
Owner EAST CHINA NORMAL UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products