[0016] Example 1, the present embodiment is made by the following raw material ratio, calculated by weight percentage: 20% dispersion resin, 1% propylene glycol ether, 0.5% 20% ammonia water, 25% deionized, 18.4% Rutile titanium dioxide, 10% superfine talc, 25% superfine calcium carbonate and 0.1% mineral oil.
[0017] Its preparation method comprises the following steps:
[0018] 1. According to the formula quantity, add the dispersed resin, propylene glycol ether, ammonia water and 2 / 3 deionized water into the stock preparation pot, stir at a low speed of 400-600rpm, and mix well;
[0019] 2. According to the amount of formula, add defoamer, after mixing evenly, add pigments and fillers: rutile titanium dioxide, superfine talc powder and superfine calcium carbonate, disperse at high speed at 1200rpm for more than 20 minutes, and form a uniform paint slurry without obvious dry powder Block;
[0020] 3. Grind the evenly stirred paint pulp until the fineness is ≤30um;
[002...
example 2
[0023] Example 2, the present embodiment is made by the following raw material ratio, calculated by weight percentage: 28% dispersion resin, 2.5% propylene glycol ether, 0.8% 20% ammonia water, 20% deionized water, 20.2% Rutile titanium dioxide, 8% ultrafine talc, 20% ultrafine calcium carbonate, 0.25% mineral oil and 0.25% polysiloxane.
[0024] Its preparation method is the same as example 1.
example 3
[0025] Example 3, the present embodiment is made by the following raw material ratio, calculated by weight percentage: 32% dispersion resin, 4% propylene glycol ether, 0.6% 20% ammonia water, 17% deionized water, 25% rutile titanium dioxide, 6% ultrafine talc, 15% ultrafine calcium carbonate, 0.134% mineral oil and 0.266% polysiloxane.
[0026] Its preparation method is the same as example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com