Waterproof corrosion-resistant heat-insulating coating

A technology of thermal insulation coating and acrylic emulsion, which is applied in the field of daily chemical industry and achieves the effects of wide application range, easy operation and easy promotion

Inactive Publication Date: 2013-04-17
YANSHAN UNIV
View PDF5 Cites 11 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] In the rapid development of my country's economy, the construction industry has been identified as the locomotive to promote sustainable economic development, and the demand for building materials is increasing day by day. , Low-end products are far from meeting the demand for quality and quantity of materials in the rapidly developing construction industry, and there is an urgent need to develop new building materials that integrate waterproof, anti-corrosion and heat preservation

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] 59g of benzene-acrylic emulsion, 5g of hollow glass microspheres, 13g of sepiolite, 8g of titanium dioxide, 2g of light calcium carbonate, 2g of Shuangfei powder, 2g of zinc white, 5g of deionized water, 1g of polyvinyl alcohol, and organosiloxane Add 0.2g, 0.7g of acid phosphate amine salt and 1g of benzimidazole ester into the reaction kettle, after emulsification and homogenization for 40 minutes, let stand for more than 3 hours, then add 0.6g of fungicide Kaison and 0.5g of narcissus essence, stir Evenly.

Embodiment 2

[0020] Mix 51g of benzene-acrylic emulsion, 8g of hollow glass microspheres, 9g of sepiolite, 5g of titanium dioxide, 5g of light calcium carbonate, 3g of Shuangfei powder, 6g of zinc white, 10g of deionized water, 0.4g of polyvinyl alcohol, and organic silicon oxide Add 0.7g of alkane, 0.4g of acidic phosphate amine salt and 0.8g of benzimidazole ester into the reaction kettle, emulsify and homogenize for 50 minutes, let it rest for more than 2.5 hours, then add 0.2g of bactericidal bactericide methylparaben, Apple essence 0.5g, just stir well.

Embodiment 3

[0022] Mix 40g of benzene-acrylic emulsion, 10g of hollow glass microspheres, 19g of sepiolite, 3g of titanium dioxide, 3g of light calcium carbonate, 4g of Shuangfei powder, 3g of zinc white, 14g of deionized water, 0.3g of polyvinyl alcohol, organic silicon oxide Add 1g of alkane, 1g of acid phosphate amine salt and 0.2g of benzimidazole ester into the reaction kettle, after emulsification and homogenization for 60 minutes, let it stand for more than 2 hours, add 1g of bactericide propyl paraben and 0.5g of strawberry essence, Just mix well.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to waterproof corrosion-resistant heat-insulating coating. The waterproof corrosion-resistant heat-insulating coating comprises the following components in percentage by weight: 40 to 60 percent of styrene-acrylate emulsion, 5 to 10 percent of hollow glass microbead, 9 to 20 percent of sepiolite, 3 to 8 percent of titanium dioxide, 1 to 5 percent of light calcium carbonate, 1 to 5 percent of heavy calcium carbonate powder, 2 to 6 percent of zinc white, 5 to 15 percent of deionized water, 0.2 to 1 percent of thickening agent, 0.2 to 1 percent of defoaming agent, 0.2 to 1 percent of antifreezing agent, 0.2 to 1 percent of preservative, 0.2 to 1 percent of bactericide and 0.5 percent of essence. The preparation method comprises the following steps: adding the styrene-acrylate emulsion, the hollow glass microbead, the sepiolite, the titanium dioxide, the light calcium carbonate, the heavy calcium carbonate powder, the zinc white, the thickening agent, the defoaming agent, the antifreezing agent and the deionized water into a reaction kettle; emulsifying and homogenizing for 40 minutes; standing for more than 2 hours; adding the bactericide and the essence; and stirring uniformly. The waterproof corrosion-resistant heat-insulating coating is non-toxic and pollution-free in raw materials and low in cost, has good waterproof, corrosion-resistant and heat-insulating effects, saves energy and reduces consumption.

Description

technical field [0001] The invention belongs to the technical field of daily chemical industry, and in particular relates to a coating for building. technical background [0002] At present, domestic roofs, roofs, pipeline waterproofing, anti-corrosion, and thermal insulation are all undertaken by different materials, and there is no one material that has two or more functions at the same time. Insulation materials mainly include polyurethane foam, perlite, silica powder, rock wool, slag, etc.; waterproof materials have developed rapidly in recent years and can be roughly divided into three categories: (1) oil-cloth waterproof materials, such as traditional petroleum asphalt felt ( Since 2000, new buildings are forbidden to use) waterproof, water-emulsion rubber asphalt felt paint waterproof, neoprene paint plus non-woven fabric waterproof, etc., the above materials not only pollute the environment, construction is troublesome, but also poor waterproof and easy to leak; ( 2...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D125/14C09D7/12C09D5/08
Inventor 于金库于美琪王跃华乔琪祝文沙康少明
Owner YANSHAN UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products