A methanol gasoline and catalyst technology, which is applied in the petroleum industry, fuel additives, liquid carbon-containing fuels, etc., can solve the problems of metal corrosion and rubber swelling, restricting the development of methanol gasoline, and small replacement ratio, and achieves overcoming high temperature non-air resistance, Overcome swelling and metal corrosion problems, clean exhaust emissions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0040] A kind of large-scale methanol gasoline catalyst, its volume percent composition is as follows:
[0041] A. Mutual solvent: 20-40% (isopropanol, n-butanol)
[0042] B. Combustion catalyst: 10-20% carbon 5 (C 5 h 12 )
[0043] C. Calorific value enhancer: 10-20% (isopropanolamine)
[0044] D. Core complex agent: 25-30% (diphosphate, dimethyl carbonate)
[0045] E. Antioxidant anti-adhesive agent: 1~5% (T-501)
[0046] F. Metal passivation agent: 1~5% (T1201)
[0047] G. Vapor pressure regulator: 1-5% (cyclohexane)
[0048] H. Rubber swelling inhibitor: 0.1~0.5%
[0049] Preparation method of the present invention:
[0050] (1) First, the diphosphate solution and the dimethyl carbonate solution are mixed in a primary mixer in a ratio of 1:1 and then mixed with isopropanol and n-butanol in an equal ratio of 1:1;
[0051] (2) carbon 5 (C 5 h 12 ) into the primary mixer;
[0052] (3) isopropanolamine is added in the primary mixer;
[0053] (4) Add T-50 in the pr...
Embodiment 2
[0059] A kind of large-scale methanol gasoline catalyst, its volume percent composition is as follows:
[0060] A. Mutual solvent: 20-40% (isopropanol, cyclohexanol)
[0061] B. Combustion catalyst: 10-20% carbon 6 (C 6 h 14 )
[0062] C. Calorific value enhancer: 10-20% (methylaniline, o-toluidine)
[0063] D. Core compounding agent: 25-30% (methyl tert-amyl ether, diisopropyl ether)
[0064] E. Antioxidant anti-adhesive agent: 1~5% (T-501)
[0065] F. Metal passivation agent: 1~5% (T1201)
[0066] G. Vapor pressure regulator: 1-5% (methyl propionate)
[0067] H. Rubber swelling inhibitor: 0.1~0.5%
[0068] Preparation method of the present invention:
[0069] (1) First, the methyl tert-amyl ether solution and the diisopropyl ether solution are mixed in a primary mixer in a ratio of 1:1 and then mixed with isopropanol and cyclohexanol in an equal ratio of 1:1;
[0070] (2) carbon 6 (C 6 h 14 ) into the primary mixer;
[0071] (3) Add methylaniline and o-toluidine ...
Embodiment 3
[0078] A kind of large-scale methanol gasoline catalyst, its volume percent composition is as follows:
[0079] A. Mutual solvent: 20-40% (isopropanol, undecyl alcohol)
[0080] B. Combustion catalyst: 10-20% carbon 8 (C 8 h 18 )
[0081] C. Calorific value enhancer: 10-20% (tetrahydrofuran)
[0082] D. Core complex agent: 25-30% (dimethyl malonate, methylene dimethyl ether)
[0083] E. Antioxidant anti-adhesive agent: 1~5% (T-501)
[0084] F. Metal passivation agent: 1~5% (T1201)
[0085] G. Vapor pressure regulator: 1 to 5% (ethylene glycol monomethyl ether)
[0086] H. Rubber swelling inhibitor: 0.1~0.5%
[0087] Preparation method of the present invention:
[0088] (1) First, the dimethyl malonate solution and the methylene dimethyl ether solution are mixed in a primary mixer in a ratio of 1:1, and then mixed with isopropanol and undecyl alcohol in an equal ratio of 1:1;
[0089] (2) carbon 8 (C 8 h 18 ) into the primary mixer;
[0090] (3) tetrahydrofuran is a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com