Environment-friendly decoration material and production process thereof
A decorative material and production process technology, applied in the field of decorative materials, can solve the problems of environmental hazards, expensive raw materials, time-consuming and labor-consuming production, etc., and achieve the effects of antibacterial and antibacterial lasting, excellent corrosion resistance, and improved adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] An environmentally friendly decorative material, comprising the following raw materials: 68g of thermoplastic acrylic resin, 30g of light calcium carbonate, 6g of nano-silver oxide, 3g of zinc oxide, 12g of bamboo charcoal fiber, 20g of epoxy tall oleate butyl ester, ethylene glycol antimony 0.8g, 2g of nonionic surfactant alkylphenol polyoxyethylene ether, 6g of antioxidant tert-butyl hydroquinone, 0.8g of silane coupling agent Si-602.
[0023] The production process of the above-mentioned environmentally friendly decorative materials comprises the following steps:
[0024] (1) Modification of thermoplastic acrylic resin: mix thermoplastic acrylic resin, nano-silver oxide, zinc oxide, antimony ethylene glycol, add appropriate amount of ethanol as solvent, add to autoclave, stir mechanically, fill nitrogen until the pressure reaches 0.2~ 0.5MPa, react at 86°C for 2.2 hours, heat up to 130°C for 1.5 hours, release gas to make the pressure reach 0.04-0.06MPa, raise the te...
Embodiment 2
[0027] An environmentally friendly decorative material, comprising the following raw materials: 70g of thermoplastic acrylic resin, 26g of light calcium carbonate, 7g of nano-silver oxide, 3g of zinc oxide, 12g of bamboo charcoal fiber, 22g of epoxy tall oleate butyl ester, ethylene glycol antimony 1.2g, nonionic surfactant fatty acid methyl ester polyoxyethylene ether 3g, antioxidant dibutyl hydroxytoluene 6g, silane coupling agent KH-570 0.8g.
[0028] The production process of the above-mentioned environmentally friendly decorative materials comprises the following steps:
[0029] (1) Modification of thermoplastic acrylic resin: mix thermoplastic acrylic resin, nano-silver oxide, zinc oxide, antimony ethylene glycol, add appropriate amount of ethanol as solvent, add to autoclave, stir mechanically, fill nitrogen until the pressure reaches 0.2~ 0.5MPa, react at 90°C for 2.8 hours, raise the temperature to 140°C for 1.6 hours, release gas to make the pressure reach 0.04-0.06M...
Embodiment 3
[0032] An environmentally friendly decorative material, comprising the following raw materials: 72g of thermoplastic acrylic resin, 36g of light calcium carbonate, 5g of nano-silver oxide, 3g of zinc oxide, 16g of bamboo charcoal fiber, 20g of epoxy tall oleate butyl ester, ethylene glycol antimony 1.1 g, 2.6 g of nonionic surfactant lauryl alcohol polyoxyethylene ether, 4 g of antioxidant tert-butylhydroquinone, and 1.2 g of silane coupling agent A-172.
[0033] The production process of the above-mentioned environmentally friendly decorative materials comprises the following steps:
[0034] (1) Modification of thermoplastic acrylic resin: mix thermoplastic acrylic resin, nano-silver oxide, zinc oxide, antimony ethylene glycol, add appropriate amount of ethanol as solvent, add to autoclave, stir mechanically, fill nitrogen until the pressure reaches 0.2~ 0.5MPa, react at 92°C for 2.2 hours, heat up to 125°C for 1.5 hours, release gas to make the pressure reach 0.04-0.06MPa, t...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com