Manufacturing method of environment-friendly five-layer plywood
A production method and technology of five-plywood, which is applied in the field of wood processing, can solve the problem of large formaldehyde released by five-plywood, and achieve the effects of improving environmental protection, providing environmental protection effects, and high bonding strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A kind of manufacturing method of environment-friendly five-ply board, comprises the following steps:
[0029] (1) Veneer drying: several veneers are dried so that the moisture content of the veneers is 5%.
[0030] (2) Embryo formation treatment: the veneers processed in step (1) are grouped into five pieces to form embryos, and the five veneers are synthesized from bottom to top into a five-ply embryo, and two adjacent veneers Glue them together with a special adhesive. The special adhesive is prepared from the following raw materials in parts by weight: 50 parts of modified phenolic glue, 20 parts of soybean protein glue, 8 parts of sodium hydroxide, 4 parts of anti-enzyme agent, 4 parts of flame retardant and 15 parts of filler . Wherein, the flame retardant is prepared from the following raw materials in parts by weight: 20 parts of chlorinated paraffin, 30 parts of ammonium oligophosphate, 10 parts of ammonium pyrophosphate and 10 parts of boric acid. The antif...
Embodiment 2
[0041] A kind of manufacturing method of environment-friendly five-ply board, comprises the following steps:
[0042] (1) Veneer drying: several veneers are dried so that the moisture content of the veneers is 10%.
[0043] (2) Embryo formation treatment: the veneers processed in step (1) are grouped into five pieces to form embryos, and the five veneers are synthesized from bottom to top into a five-ply embryo, and two adjacent veneers Glue them together with a special adhesive. The special adhesive is prepared from the following raw materials in parts by weight: 60 parts of modified phenolic glue, 30 parts of soybean protein glue, 12 parts of sodium hydroxide, 8 parts of anti-enzyme agent, 8 parts of flame retardant and 20 parts of filler . Wherein, the flame retardant is prepared from the following raw materials in parts by weight: 30 parts of chlorinated paraffin, 40 parts of ammonium oligophosphate, 16 parts of ammonium pyrophosphate and 16 parts of boric acid. The ant...
Embodiment 3
[0054] A kind of manufacturing method of environment-friendly five-ply board, comprises the following steps:
[0055] (1) Veneer drying: several veneers are dried so that the moisture content of the veneers is 8%.
[0056] (2) Embryo formation treatment: the veneers processed in step (1) are grouped into five pieces to form embryos, and the five veneers are synthesized from bottom to top into a five-ply embryo, and two adjacent veneers Glue them together with a special adhesive. The special adhesive is prepared from the following raw materials in parts by weight: 55 parts of modified phenolic glue, 25 parts of soybean protein glue, 10 parts of sodium hydroxide, 6 parts of anti-enzyme agent, 6 parts of flame retardant and 17 parts of filler . Wherein, the flame retardant is prepared from the following raw materials in parts by weight: 25 parts of chlorinated paraffin, 35 parts of ammonium oligophosphate, 13 parts of ammonium pyrophosphate and 13 parts of boric acid. The anti...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com