Fire coal clean assistant and preparation method thereof
A cleaning aid, coal-burning technology, used in fuel, solid fuel, petroleum industry and other directions, can solve the problems of inability to carry out harmful gases, many harmful gases, and large pollution, achieve clean and non-toxic raw materials, reduce environmental pollution, and prepare simple method effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0032] Another object of the present invention lies in a kind of preparation method of coal-fired cleaning aid, comprising the following steps:
[0033] A. Add 0.5-1.5 parts by weight of composite adhesive to 4-7 parts by weight of water, mix and stir, add 0.5-1.5 parts by weight of titanium dioxide, and mix well to obtain liquid A;
[0034] B. Add 2 to 4 parts by weight of calcium magnesium acetate into 4 to 8 parts by weight of water, and stir evenly to obtain liquid B;
[0035] C. Mix 1-5 parts by weight of calcium oxide, 1-3 parts by weight of urea, and 0.5-1.5 parts by weight of catalyst to obtain powder C;
[0036] D. Mix powder C and liquid B, then add liquid A, after mixing, enter the mixer and stir for 1 to 2 hours to obtain an environmentally friendly coal-fired cleaning aid.
[0037] Preferably, the calcium magnesium acetate is mixed with calcium acetate and magnesium acetate at a mass ratio of 3:1, and then mixed with a magnesium chloride solution with a mass conc...
Embodiment 1
[0041] Weigh 100g of compound modified starch and add it to 600g of water, mix and stir, add 75g of titanium dioxide, fully stir for 10min, mix well and get liquid A for later use;
[0042] Add 200g of calcium magnesium acetate to 600g of water and stir for 5 minutes to obtain liquid B for later use;
[0043] Fully mix 500g of calcium oxide, 300g of urea, and 150g of catalyst to obtain powder C;
[0044] Mix powder C and liquid B, then add liquid A, after mixing, enter the mixer and stir for 1 to 2 hours to obtain an environmentally friendly coal-fired cleaning aid.
[0045] Add 7% (i.e. 2.52kg) of the above-mentioned environmentally friendly coal-fired cleaning additives to 36kg of coal-fired coal. The above-mentioned 2.52kg of clean coal-fired additives are evenly mixed with 36kg of coal powder, and the coal is pressed into shape, and then burned on the stove Internal combustion, the combustion temperature is controlled at about 900°C. After combustion tests and tests, when...
Embodiment 2
[0048] Weigh 150kg of polyvinyl alcohol and add it to 1000kg of water, mix and stir, add 150kg of titanium dioxide, fully stir for 10min, and mix well to obtain liquid A for later use;
[0049] Add 500kg of calcium magnesium acetate into 300kg of water and stir for 5 minutes to obtain liquid B for subsequent use;
[0050] The calcium oxide of 100kg, the urea of 150kg, the catalyst of 75kg are fully mixed, obtain powder C;
[0051] Mix powder C and liquid B, then add liquid A, after mixing, enter the mixer and stir for 1 to 2 hours to obtain an environmentally friendly coal-fired cleaning aid.
[0052] Add 10% (i.e. 10kg) of the above-mentioned environmentally friendly coal-fired cleaning additives to 1000kg of coal-fired coal. The above-mentioned 10kg of clean coal-fired additives are evenly mixed with 1000kg of coal powder, and the coal is pressed into shape, and then burned in the combustion stove , the combustion temperature is controlled at 1000°C. After combustion test...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com