Graphene-based cigarette paper and preparation method thereof
A graphene-based, cigarette paper technology, applied in paper, papermaking, paper coating, etc., can solve the problems of not being able to give personalized visual effects at the same time, short retention time of flavor substances, and affecting the quality of cigarette products, so as to improve the quality of cigarette products , prolong the retention time, and avoid the pollution of the workshop environment and equipment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] (1) Weigh 500 g of graphene oxide, soak it in 5 L of deionized water / ethanol mixed solvent (V / V=5:1) for 2 h, and ultrasonicate for 0.5 h at room temperature in an ultrasonic device with a power of 100 W to obtain Uniformly dispersed graphene oxide dispersion; wherein, the sheet size of graphene oxide is 10-20 μm, the thickness is 2.0-4.0 nm, and the C / O is 3:1;
[0032] (2) Add 50 g of glycerol humectant, 100 g of coffee arabica extract, and 5 g of tea polyphenols to the graphene oxide dispersion obtained in step (1), stir evenly for 1.5 h, and mix well. Obtain graphene functional compound after homogeneous;
[0033] (3) Spin-coat the graphene functional composite obtained in step (2) on the surface of cigarette paper, and the coating amount is 10g / m of graphene composite 2 , and then dried at 110 °C for 1 min to obtain graphene-based cigarette paper. According to the conventional cigarette paper processing technology, the upper rolling machine is used for cigarette ...
Embodiment 2
[0036] (1) Weigh 350 g of graphene oxide, soak it in 1 L of deionized water / propylene glycol mixed solvent (V / V=7 / 2) for 2 h, and ultrasonicate at room temperature for 1 h in an ultrasonic device with a power of 100 W. Obtain a uniformly dispersed graphene oxide dispersion; wherein, the sheet size of graphene oxide is 13-18 μm, the thickness is 2.5-3.5 nm, and the C / O is 3:1; (2) the oxidized Add 10 g combustion enhancer sodium citrate, 20 g honey humectant, 500 g Dali plum extract, and 20 g taste regulator citric acid to the graphene dispersion, stir evenly for 2 h, and obtain graphene functional compound after fully mixing thing;
[0037] (3) Spray the graphene composite obtained in step (2) on the surface of the cigarette paper, and the coating amount is 5 g / m of the graphene composite 2 , and then dried at 110 °C for 30 s to obtain graphene-based cigarette paper. According to the conventional cigarette paper processing technology, the upper rolling machine is used for ci...
Embodiment 3
[0040] (1) Weigh 1 kg of graphene oxide, soak it in 9 L of deionized water / ethanol / propylene glycol (V / V=6 / 1) for 2 h, and ultrasonicate for 2.5 h at room temperature in an ultrasonic device with a power of 100 W. Obtain a uniformly dispersed graphene oxide dispersion; wherein, the sheet size of graphene oxide is 10-20 μm, the thickness is 2.0-4.0 nm, and the C / O is 3:1; (2) the oxidized Add 2 kg of Rosa roxburghii extract, 20 g of sodium citrate as a combustion enhancer, 50 g of tobacco polysaccharide humectant, and 10 g of dextran as a sweetener to the graphene dispersion, stir for 1.5 h, and mix thoroughly to obtain graphite ene functional complexes;
[0041] (3) Spray the graphene composite obtained in step (2) on the surface of the cigarette paper according to the designed auspicious cloud pattern, and the coating amount is 7 g / m of graphene composite 2, and then dried at 110 °C for 10 s to obtain graphene-based cigarette paper applications. According to the conventiona...
PUM
Property | Measurement | Unit |
---|---|---|
size | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com